Spectrum from Mexico

Postby BobbieMatus » Wed Nov 15, 2017 8:54 am

Has anyone used spectrum coming from Oceanside (mexico). I'm wondering about quality

Brad Walker
Site Admin
Posts: 1385
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Spectrum from Mexico

Postby Brad Walker » Wed Nov 15, 2017 10:07 am

Haven't used any personally, but we've heard mixed reviews. Some say it's ok, some say it's not as good as the original.


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 70 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com