Postby mikefromitaly » Wed Apr 25, 2018 5:38 am

Hello friends,

during a fusing the window of my paragin sc2 with door and window become black and i am not able to see inside anymore?

what do you think happened?..and any way to restore the glass to look again inside?

thanks for support and collaboration,

mike
thanks for sharing !

mike from italy


"secret of success?... passion & experience"

[url] http://www.picturetrail.com/mikefromitaly [/url]

Joyce Walters
Posts: 80
Joined: Thu Nov 08, 2007 12:06 am
Location: Stevensville MT

Re: paragon window

Postby Joyce Walters » Fri Apr 27, 2018 3:15 pm

Hi Mike.
Do you know what caught on fire in the kiln?
Maybe it was just smoke from the kiln paper not vented?
Joyce from MT

Ed Cantarella
Posts: 155
Joined: Mon Feb 26, 2018 3:49 pm
Location: Highland, Michigan, USA

Re: paragon window

Postby Ed Cantarella » Mon Apr 30, 2018 11:54 am

After trying to clean it, maybe try a little cerium oxide with a wet cloth. To polish the surface. Hopefully it is not ruined. :cry:
HER last words were, "I'm melting, melting . . . " Dissenting opinions generally welcome for comic relief or personal edification. Sometimes both.

mikefromitaly
Posts: 67
Joined: Thu Apr 03, 2003 7:47 am
Location: italy-sicily
Contact:

Re: paragon window

Postby mikefromitaly » Mon Apr 30, 2018 2:22 pm

Hi
Thank you.
I used thinfire paper of bullseye..and you are right.. Maybe was the fumes not vented.
It was not easy to clean but i did in the end.
So in which case i have to vent the kiln? And how?
(My paragon has a cone on the top?)
Thanks for your support and collaboration
Mike
thanks for sharing !

mike from italy


"secret of success?... passion & experience"

[url] http://www.picturetrail.com/mikefromitaly [/url]


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: Majestic-12 [Bot] and 41 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com

cron