Schedule for kiln pressed glass - for Uroboros

Posted: Sat Apr 24, 2021 4:10 pm
by Havi
Hello everybody,
I discovered a nice pack of Uroboros glass in my storage.
Some of it is very nice colors.Eventhough its COE is 90 - it is fired on different schedule than BE.

Being weak in numbers, I would appreciate it if anybody could refer me to Uroboros firing schedule for SMOOSHED GLASS, or UNDER PRESSURE or KILN PRESSED GLASS - those are all names of the same process.

I'd be more than grateful!!!


Havi

Re: Schedule for kiln pressed glass - for Uroboros

Posted: Sat Apr 24, 2021 9:02 pm
by Brad Walker
I never fired Uro 90 that much (if any) different than Bullseye. The same schedule ought to work.

Re: Schedule for kiln pressed glass - for Uroboros

Posted: Sun Apr 25, 2021 1:59 am
by Havi
Thank, Brad

My best teacher!

Did you also mix BE AND URO????

many thanks in advance

H

Re: Schedule for kiln pressed glass - for Uroboros

Posted: Sun Apr 25, 2021 8:44 am
by Brad Walker
Havi wrote:Did you also mix BE AND URO????
Always the clear Uro with BE, no problems. Sometimes the other colors. Only problem I ever experienced was with one of the Uroboros reds. Not surprising since reds can be difficult to make.

Re: Schedule for kiln pressed glass - for Uroboros

Posted: Mon Apr 26, 2021 3:28 pm
by Havi
Thanks a lot, Brad

Always appreciate your knowledge,
and
your
sharing it!!!