Any suggestions for a clear glass (Bullseye coe 90) as a fused topping glass? Need clear and no bubbles.
david n
Posts: 34
Joined: Mon Dec 03, 2007 12:24 am
Location: Akron, Ohio
Contact:

Re: best glass for toppping

Post by david n »

I use 3mm Tekta clear to cap all of my work. Bullseye also makes crystal clear Tekta, but the regular works well for me. Occasionally I find bubbles that I don't like and I will just drill them out and use the piece on a different layer of my work.
Birdzilla44
Posts: 7
Joined: Mon Jan 25, 2021 10:56 am

Re: best glass for toppping

Post by Birdzilla44 »

Thanks David. I have not tired the crystal clear tekta, but if the difference is negligible in clarity and lack of color, the regular should work for me. A good shiny clear is want I want.