Fusing 5mm clear sheets

Posted: Tue Jun 21, 2022 8:09 pm
by Peter Zelle
Hi,
I am running out of COE 96 casting plates and cannot find anymore. Sadness.
My castings are 6 to 7 feet tall and about 1.5 thick with frit on the surface of the mold.
Thinking of fusing 8 layers of 5mm clear sheets together.
Is this crazy or worth a try?
Appreciate any thoughts or info your can share,
Thanks, Peter

Re: Fusing 5mm clear sheets

Posted: Thu Jun 23, 2022 5:59 pm
by Kevin Midgley
Switch to Bullseye glass.
Yes you can fuse sheets together however inevitably there will be bits of 'stuff like studio dust' between the layers.

Re: Fusing 5mm clear sheets

Posted: Mon Sep 26, 2022 11:43 pm
by Terry Gallentine
Peter--Did you go ahead and experiment with fusing multiple layers of 5mm clear together? If you did, did you use the Oceanside 96 or did you use the Wissmach 96? I am thinking about trying out the Wissmach 96 and might be interested in putting together an order with someone else for some full sheets (32"x42").