I have some resiprators from work.
The guys wear them that scale the
ingrediants and load the mixers
Niosh N95
Some of the stuff these guys scale up
is pretty icky .....will these work for
blasting in a cabinet?
respirator # N95
Moderators: Brad Walker, Tony Smith
-
Amy Schleif-Mohr
- Posts: 280
- Joined: Sun Mar 09, 2003 5:18 pm
- Location: Milwaukee
-
Greg Rawls
- Posts: 147
- Joined: Sun Mar 09, 2003 8:11 pm
- Location: Charleston, SC
- Contact:
N95 is prefectly adequate for sandblasting. We did a study on N95 vs P100 for exposure to a carcinogen at work and found the N95 to be more than adequate. Actually, you can use a filtering facepiece - that's a disposable respirator for dust.
The difference between P100 and N95 all goes to how NIOSH tests respirators. Check my web site for more information on respirators.
Greg the Certified Industrial Hygienist
http://www.gregorieglass.com
The difference between P100 and N95 all goes to how NIOSH tests respirators. Check my web site for more information on respirators.
Greg the Certified Industrial Hygienist
http://www.gregorieglass.com
Greg
I wondered, because the ingrediants used in industrial baking are pretty fierce not to mention fine. These have a little plastic intake / outtake valve on them. White lung being a common ailment in baking, I had hoped these were up to the task. I had hoped if not for blasting, then preparing shelves and cutting fiberboard. I apreciate all feedback...specially when my health is involved. And the new cabinet should not leak quick so badly...
one would hope.
one would hope.
-
Greg Rawls
- Posts: 147
- Joined: Sun Mar 09, 2003 8:11 pm
- Location: Charleston, SC
- Contact:
What is the grit you are using? I'm assuming you are using aluminum oxide or silicon carbide. NEVER use sand or any grit that contains SILICA in a sandblaster unless you have an excellent dust collection system, the cabinet does not leak and you are wearing a P100 fullface respirator!!! (Did is scare you enough? Silica is serious stuff!).
Greg
just say no to silica
I am using 100 grit aluminum oxide.
my new cabinet will have a vacuum.
my new cabinet will have a vacuum.
-
Greg Rawls
- Posts: 147
- Joined: Sun Mar 09, 2003 8:11 pm
- Location: Charleston, SC
- Contact: