Postby Tony Serviente » Thu Mar 25, 2004 9:56 am

Just had the opportunity to look at the safety section of Gregs site, and would like to thank him for making the information not only easy to understand, but to have put it in the context of hot and warm glass. While safety consciousness is higher now than I have seen it, many of the materials we work with on a daily basis are still treated cavalierly. I know that making the pages to present the info was no half hour job, so particularly appreciate his selflessness. Thanks Greg!

barbarak
Posts: 22
Joined: Thu Mar 04, 2004 11:30 am
Location: Just east of being there.

Link to Greg Rawl's site

Postby barbarak » Thu Mar 25, 2004 1:38 pm

Would you share the link to his site? I love to take a look at it. Thanks.
Barbara

Tony Serviente
Posts: 328
Joined: Thu May 29, 2003 11:48 am
Location: Ithaca,NY
Contact:

Postby Tony Serviente » Thu Mar 25, 2004 1:46 pm


Carole Burton
Posts: 38
Joined: Mon Mar 10, 2003 12:57 pm
Location: Charleston, S.C.

Thanks to Greg Rawls

Postby Carole Burton » Thu Mar 25, 2004 1:51 pm

Tony... I agree totally agree with everything you said about Greg's Safety Website. Many of us non-chemically trained fuser are aware of the safety issues that are involved with fusing glass but are not quite sure how to go about protecting ourselves. Thanks for taking the time to create the nice website and simply spelling out what to do to keep ourselves healthy.

You done good Greg...... Thanks.
.
Carole...S.C.

Carole Burton
Posts: 38
Joined: Mon Mar 10, 2003 12:57 pm
Location: Charleston, S.C.

Thanks to G R

Postby Carole Burton » Thu Mar 25, 2004 1:59 pm

Try www. gregorieglass.com

Sorry can't figure out how to do it blue..

Carole....S.C.

Carole Burton
Posts: 38
Joined: Mon Mar 10, 2003 12:57 pm
Location: Charleston, S.C.

Thanks to G R

Postby Carole Burton » Thu Mar 25, 2004 2:35 pm

Try www. gregorieglass.com

Sorry can't figure out how to do it blue..

Carole....S.C.

travisraybold
Posts: 25
Joined: Tue Jan 20, 2004 12:10 pm
Location: Portland, OR
Contact:

Postby travisraybold » Thu Mar 25, 2004 3:41 pm

this is a great to have a summary of the safety issues available! ive been debating what steps to take first in making my studio a safe one, and this list helps me a lot.

is the kiln wash you scrape off after firing just "nusiance dust", or do i need to take it outside, wear a respirator, and vacuum it witth a hepa shark? right now im just scraping it off on a table and using my shop vac (waiting for a hepa shark to come in).

im planning on trying to avoid using fiber paper whenever possible, as im assuming kiln wash is a safer alternative, is that generally assumed to be correct?

thanks,

--travis

Greg Rawls
Posts: 147
Joined: Sun Mar 09, 2003 8:11 pm
Location: Charleston, SC
Contact:

Postby Greg Rawls » Thu Mar 25, 2004 8:26 pm

WOW! Ya'll are way to kind! Thank you! Being a safety and health "geek" and a di-hard glass fuser, I'm glad to share 20 years of experience in the industrial hygiene, toxicology and safety field!

Travis- kiln wash that you scrap off a kiln shelf would be considered nuisance dust. When I'm just scraping, I don't bother with a respirator as the stuff does not become airborne and respirable. However, sometimes I need to sand and then I put on a dust respirator and turn on my Shopvac with HEPA filter to keep the dust under control.
Greg

Judith Andre
Posts: 28
Joined: Thu Mar 20, 2003 2:38 am
Location: Lincoln, NE

Postby Judith Andre » Sat Mar 27, 2004 5:32 pm

Good information. Thanks! How about a section on eye protection?

Judith
Judith

Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Postby Bert Weiss » Sun Mar 28, 2004 12:32 am

Greg Rawls wrote:WOW! Ya'll are way to kind! Thank you! Being a safety and health "geek" and a di-hard glass fuser, I'm glad to share 20 years of experience in the industrial hygiene, toxicology and safety field!

Travis- kiln wash that you scrap off a kiln shelf would be considered nuisance dust. When I'm just scraping, I don't bother with a respirator as the stuff does not become airborne and respirable. However, sometimes I need to sand and then I put on a dust respirator and turn on my Shopvac with HEPA filter to keep the dust under control.


Can aybody recommend a decent hepa filter shop vac? How much do you have top spend?
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions

Lauri Levanto
Posts: 270
Joined: Tue Mar 11, 2003 7:33 am
Location: Halikko, Finland

Postby Lauri Levanto » Sun Mar 28, 2004 3:16 am

Thanks Gred

for a wealth of sober information.
May I include a link in the WG dictionary
under safety?

-lauri

Greg Rawls
Posts: 147
Joined: Sun Mar 09, 2003 8:11 pm
Location: Charleston, SC
Contact:

Postby Greg Rawls » Sun Mar 28, 2004 9:30 am

>>>Can aybody recommend a decent hepa filter shop vac? How much do you have top spend?

Go to Lowes/Home Depot. They make HEPA filter for Shop Vacs.

>>>Thanks Gred for a wealth of sober information. May I include a link in the WG dictionary under safety?

Sure! "Gred" aka "Greg"
Greg

Tony Serviente
Posts: 328
Joined: Thu May 29, 2003 11:48 am
Location: Ithaca,NY
Contact:

Postby Tony Serviente » Mon Mar 29, 2004 9:16 am

Bert-Sears also sells them. I have a couple of big Sears shop vacs and have used their Hepa fillters for a while, with good results.


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 28 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com

cron