Post by Judy Schnabel »

I just finished reading the thread on duraboard firing.

I applied the rigidized on all six sides; let it dry for two days; fired it to 1450. I opened the kiln this morning and the board is all blotchy. Charlie says if it's not white, flip it over and fire it again.

I flipped it over and the other side is all blotchy also.

Is this thing suppose to end up white or did I not put enough rigidizer on it?

Judy
Phil Hoppes
Posts: 298
Joined: Wed Mar 12, 2003 2:20 pm
Location: Overgaard, AZ

Post by Phil Hoppes »

Fire it again. It usually takes a couple of firings to clean it up.

Phil
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Duraboard

Post by Bert Weiss »

Judy Schnabel wrote:I just finished reading the thread on duraboard firing.

I applied the rigidized on all six sides; let it dry for two days; fired it to 1450. I opened the kiln this morning and the board is all blotchy. Charlie says if it's not white, flip it over and fire it again.

I flipped it over and the other side is all blotchy also.

Is this thing suppose to end up white or did I not put enough rigidizer on it?

Judy
White means that the binders are burned out. Blotchy, not quite burned out.

The way I have always approached burnout is to fire to whatever temp you plan to use the board at. If you are a comber, go to 1700. If you fire at 1500, go there...
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Judy Schnabel
Posts: 195
Joined: Mon Mar 10, 2003 9:45 pm
Location: SW FL
Contact:

Post by Judy Schnabel »

Thanks Phil & Bert,

I'll crank it up again.