Postby lbailey » Sat Apr 26, 2014 9:04 am

Are fused glass items with the Irid side up food safe?

I suspect that energetic use of tableware will mar the finish and probably lifts bits of the irid coating to add "flavor" to the food.......?

How about for use with food but no tableware touching, like a dish for hard candy?

Thanks

Brad Walker
Site Admin
Posts: 1385
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Irid Food Safe?

Postby Brad Walker » Sat Apr 26, 2014 1:24 pm

Bullseye irid is food safe. Not sure about other brands, there are several different ways to apply the irid coating.

It's pretty hard to remove the irid coating with a knife and fork.

Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: Irid Food Safe?

Postby Valerie Adams » Sat Apr 26, 2014 1:54 pm

I tell customers to use their fused glass like they'd use fine china dinnerware, which means no knives. I'm always stunned when someone purchases one of my pieces and plans to eat off it though, since I can't imagine spending a few hundred bucks on a piece and then plopping a steak on it, but hey, once they've paid I guess it's theirs to do what they want.

lbailey
Posts: 86
Joined: Fri Oct 26, 2012 2:53 pm
Location: FL Panhandle

Re: Irid Food Safe?

Postby lbailey » Sat Apr 26, 2014 4:03 pm

Thanks guys, good to know.

JestersBaubles
Posts: 698
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: Irid Food Safe?

Postby JestersBaubles » Sun Apr 27, 2014 12:13 am

Valerie, I feel the same way when someone asks me if they can put a piece in the dishwasher.

Really? You're going to pay THAT much for a bowl and then put it in the dishwasher??

Dana W.

Greg Rawls
Posts: 147
Joined: Sun Mar 09, 2003 8:11 pm
Location: Charleston, SC
Contact:

Re: Irid Food Safe?

Postby Greg Rawls » Sun Apr 27, 2014 8:04 am

Greg

Judd
Posts: 291
Joined: Mon Sep 01, 2003 9:45 am
Location: Arkansas

Re: Irid Food Safe?

Postby Judd » Mon Apr 28, 2014 1:13 pm

I tell my customers, yes it's dishwasher safe but I would never put it in the dishwasher.

Terry Ow-Wing
Posts: 124
Joined: Sun Mar 09, 2003 3:21 pm
Location: San Francisco, Ca.
Contact:

Re: Irid Food Safe?

Postby Terry Ow-Wing » Mon Apr 28, 2014 5:04 pm

Yes it can go into the dishwasher but do you normally put art into the dishwasher? Then if that doesn't work I tell them that when you put things in the dishwasher all your plates are the same and so when they move around they do it in unison - if you have an shape that doesn't match all the other plates it could be the full weight swing right at your art piece. After this I give up..... #-o
Terry Ow-Wing Designs
Kilnformed and Lampworked Glass Art
http://GlassArt.weebly.com
Image

nbobb
Posts: 25
Joined: Mon Aug 16, 2004 1:35 pm
Location: California
Contact:

Re: Irid Food Safe?

Postby nbobb » Thu May 01, 2014 6:08 pm

I have a Pyrex measuring cup that I've had for years. It became crazed in the dishwasher because some soaps are very abrasive. If I took a sandblaster to an iridized plate that was already fused, I could blow off the irid and I think, over time, the dishwasher could do the same thing.
Nancy Bobb
Firewalker Studio
http://www.firewalkerstudio.com

lbailey
Posts: 86
Joined: Fri Oct 26, 2012 2:53 pm
Location: FL Panhandle

Re: Irid Food Safe?

Postby lbailey » Thu May 01, 2014 7:48 pm

Yeah, I tell customers that the plates/bowls are food safe but not for the microwave or dishwasher, hand wash only. I suspect most pieces would survive on the top rack but hey, if you can't hand wash something unique then you don't need to buy it......


Post Reply

Return to “Newcomer Forum”

Who is online

Users browsing this forum: No registered users and 8 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com