Hi.
i would like to know how to cut Grafite Plates.
thank you
mike
graphite
Moderator: Tony Smith
-
mikefromitaly
- Posts: 67
- Joined: Thu Apr 03, 2003 7:47 am
- Location: italy-sicily
- Contact:
graphite
thanks for sharing !
mike from italy
"secret of success?... passion & experience"
http://www.picturetrail.com/mikefromitaly
mike from italy
"secret of success?... passion & experience"
http://www.picturetrail.com/mikefromitaly
Re: graphite
you buy them. it depends upon how big you need. marble or bead makers use them. you can probably get them off ebay cheaply.
-
Brad Walker
- Site Admin
- Posts: 1539
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: graphite
A diamond saw blade will cut graphite.mikefromitaly wrote:i would like to know how to cut Grafite Plates.
-
The Hobbyist
- Posts: 311
- Joined: Sun Mar 09, 2003 7:09 pm
- Location: Sun City West (NW Phoenix), AZ
- Contact:
Re: graphite
Graphite machines very nicely with nearly any cutting tool, even hand tools. The big problem is handling the shavings. When I work it I keep a vacuum constantly cleaning the cutting site so they don't fall or float about.
Jim "The Hobbyist"
Jim "The Hobbyist"
"With or without religion, good people can behave well and bad people can do evil; but for good people to do evil—that takes religion. " Steven Weinberg
-
Sean McFeely
- Posts: 3
- Joined: Thu Jul 23, 2015 9:52 am
Re: graphite
I agree with the hobbyist. If you are not careful to manage the dust you can and will short out your bushings on your electric motors as the dust is a conductor.