Hi.
i would like to know how to cut Grafite Plates.

thank you

mike
thanks for sharing !

mike from italy


"secret of success?... passion & experience"

[url] http://www.picturetrail.com/mikefromitaly [/url]

charlie
Posts: 961
Joined: Mon Mar 10, 2003 3:08 pm

Re: graphite

Postby charlie » Wed Feb 25, 2015 12:05 am

you buy them. it depends upon how big you need. marble or bead makers use them. you can probably get them off ebay cheaply.

Brad Walker
Site Admin
Posts: 1380
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: graphite

Postby Brad Walker » Wed Feb 25, 2015 12:23 pm

mikefromitaly wrote:i would like to know how to cut Grafite Plates.


A diamond saw blade will cut graphite.

The Hobbyist
Posts: 303
Joined: Sun Mar 09, 2003 7:09 pm
Location: Sun City West (NW Phoenix), AZ
Contact:

Re: graphite

Postby The Hobbyist » Wed Feb 25, 2015 12:50 pm

Graphite machines very nicely with nearly any cutting tool, even hand tools. The big problem is handling the shavings. When I work it I keep a vacuum constantly cleaning the cutting site so they don't fall or float about.

Jim "The Hobbyist"
"With or without religion, good people can behave well and bad people can do evil; but for good people to do evil—that takes religion. " Steven Weinberg

Sean McFeely
Posts: 3
Joined: Thu Jul 23, 2015 9:52 am

Re: graphite

Postby Sean McFeely » Thu Aug 06, 2015 4:26 pm

I agree with the hobbyist. If you are not careful to manage the dust you can and will short out your bushings on your electric motors as the dust is a conductor.


Post Reply

Return to “Newcomer Forum”

Who is online

Users browsing this forum: No registered users and 6 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com