Boron Nitride POWDER

Post by Jan de Jong »

I found this question here from long ago, but there was no response.
Boron Nitride spray is used as seperator on RVS.
But there is also POWDER. Had anyone try this ?? Jan
jim simmons
Posts: 478
Joined: Sun Mar 09, 2003 10:37 pm
Location: Hillsboro Oregon
Contact:

Re: Boron Nitride POWDER

Post by jim simmons »

Mix the powder with water to a cream consistency and paint it on like you would kiln wash.
I have used it on SS and clay fired stuff with good results.
The other Jim
Jan de Jong
Posts: 114
Joined: Sun Mar 09, 2003 3:31 pm
Location: The Netherlands

Re: Boron Nitride POWDER

Post by Jan de Jong »

@ Jim Simmons: Thank you for your reply !! Do you heat the SS ( and Clay fired) ?? Jan
jim simmons
Posts: 478
Joined: Sun Mar 09, 2003 10:37 pm
Location: Hillsboro Oregon
Contact:

Re: Boron Nitride POWDER

Post by jim simmons »

nope. treat it just like it is a product called "ZYP".
paint it on, let it dry for about 30 min. and you are good to go.
The Other Jim
Jan de Jong
Posts: 114
Joined: Sun Mar 09, 2003 3:31 pm
Location: The Netherlands

Re: Boron Nitride POWDER

Post by Jan de Jong »

@ Jim: Thank you ! I PM you for another question. Jan