BE opaline strike temp

This forum is for questions from newcomers to kiln-forming.

Moderator: Tony Smith

Post Reply
jim simmons
Posts: 478
Joined: Sun Mar 09, 2003 10:37 pm
Location: Hillsboro Oregon
Contact:

BE opaline strike temp

Post by jim simmons »

I have some BE Opaline striker and need to know what temp to take it to so that it strikes.
Thanks
The other Jim
Jan de Jong
Posts: 114
Joined: Sun Mar 09, 2003 3:31 pm
Location: The Netherlands

Re: BE opaline strike temp

Post by Jan de Jong »

Jim, no answers so I decided to try to help you but I am not sure you mean this! Bullseye site: Opaline striker....Full fuse. Jan