freeze fuse with transparent

Post by Michael Stevens »

I've made some nice silicon molds and made some nice opaque castings with freeze and fuse but is there anyway to get a more transparent cast? mix fine frit with powder?
Barry Kaiser
Posts: 307
Joined: Mon Jul 25, 2005 6:54 pm
Location: North Carolina
Contact:

Re: freeze fuse with transparent

Post by Barry Kaiser »

Nope,
Won't get clear pieces.
Trapped air greys the frit.