glass I'm working on - WarmGlass.com

glass I'm working on

Want to share a photo of your work? Or get feedback on a new piece? Post it here. (Note: items in this forum are deleted periodically, generally after several months.)

Moderator: Brad Walker

Post Reply
Don Burt
Posts: 559
Joined: Sun Mar 09, 2003 8:45 pm
Location: Cincinnati, Ohio
Contact:

glass I'm working on

Postby Don Burt » Fri Jan 05, 2018 9:54 pm

IMG_0010_small.jpg

IMG_1533_small.jpg

Some bullseye tack fusing and carving in the flowers.

linn keller
Posts: 52
Joined: Mon Mar 10, 2003 12:22 pm
Location: south tx

Re: glass I'm working on

Postby linn keller » Sat Jan 06, 2018 11:04 am

don,
gorgeous!
is it for you or some lucky other?
thanks for posting pics; always a treat to see what you're working on.
linn
linn in deep deep south texas

Kevin Midgley
Posts: 742
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: glass I'm working on

Postby Kevin Midgley » Sat Jan 06, 2018 12:42 pm

Beautiful =D>
The panel edges are they etched flashed glass?
They are spectacular.

Vonon
Posts: 191
Joined: Fri Mar 10, 2006 6:32 pm
Location: East Tennessee

Re: glass I'm working on

Postby Vonon » Sat Jan 06, 2018 1:02 pm

Spectacular is the word! Your work is unlike any other and I'm impressed by the ever increasing degree of difficulty. I was waiting for a sun catcher photo but this is so much more satisfying! =D>
Vonon

Don Burt
Posts: 559
Joined: Sun Mar 09, 2003 8:45 pm
Location: Cincinnati, Ohio
Contact:

Re: glass I'm working on

Postby Don Burt » Sat Jan 06, 2018 7:54 pm

Thank you for the compliments. Those blue on white border pieces are screen printed enamels on float glass, sandblasted on the back. Its the biggest single installation I've ever attempted. Got a long way to go. Fun though.

Don Burt
Posts: 559
Joined: Sun Mar 09, 2003 8:45 pm
Location: Cincinnati, Ohio
Contact:

Re: glass I'm working on

Postby Don Burt » Sat Jan 06, 2018 7:56 pm

linn keller wrote:don,
gorgeous!
is it for you or some lucky other?
thanks for posting pics; always a treat to see what you're working on.
linn

Thanks Linn. These are for a family member's home out in Tucson.

Marty
Posts: 857
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: glass I'm working on

Postby Marty » Sat Jan 06, 2018 10:38 pm

Don- Are you taking applications for new family members?

Don Burt
Posts: 559
Joined: Sun Mar 09, 2003 8:45 pm
Location: Cincinnati, Ohio
Contact:

Re: glass I'm working on

Postby Don Burt » Sun Jan 07, 2018 4:30 pm

No Marty, I have enough family to keep me busy for now. They've been great patrons over the years though. Patient with my slow output. I'm hoping to step up the pace since I retired recently but life has a way of getting in the way.

Buttercup
Posts: 585
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: glass I'm working on

Postby Buttercup » Sun Jan 07, 2018 10:27 pm

Beautiful intricate work, Don, and a few more steps up the degree-of-difficulty scale. Thanks for sharing, Jen

JestersBaubles
Posts: 700
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: glass I'm working on

Postby JestersBaubles » Tue Jan 09, 2018 11:25 pm

Beautiful. I, too, would like to apply for family membership!

Dana W.

Nikki ONeill
Posts: 169
Joined: Mon Mar 10, 2003 11:55 am
Location: Silver Spring, MD
Contact:

Re: glass I'm working on

Postby Nikki ONeill » Sun Feb 25, 2018 1:12 pm

Lovely work, Don.

Don Burt
Posts: 559
Joined: Sun Mar 09, 2003 8:45 pm
Location: Cincinnati, Ohio
Contact:

Re: glass I'm working on

Postby Don Burt » Mon Feb 26, 2018 9:57 pm

Thank you. Making slow progress here on the project. Two of the eventual four sections are pretty much complete. The arched sections will actually be on top, with the square panels on the bottom, in the eventual setting.
Image

Buttercup
Posts: 585
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: glass I'm working on

Postby Buttercup » Tue Feb 27, 2018 2:41 am

I'm running out of superlatives here, Don. Is the blue enamel R&G transparent? It's so intense, not wishy-washy at all. Is it the sandblasting on the back that contributes to the intensity? I can get reasonable results on white but on clear glass the effect is pretty blah. I don't have R&G enamels though, because of the lifetime-supply minimum quantities.

Are you sandblasting before firing so the etched glass gets a fire-polish as well? They are gorgeous whatever you're doing! Jen

Havi
Posts: 603
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Re: glass I'm working on

Postby Havi » Tue Feb 27, 2018 5:52 am

Like the ones before me, I run out of words.
This is so very beautiful - - -
Good for you!


Many thanks for sharing!

Havi
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com

Don Burt
Posts: 559
Joined: Sun Mar 09, 2003 8:45 pm
Location: Cincinnati, Ohio
Contact:

Re: glass I'm working on

Postby Don Burt » Tue Feb 27, 2018 8:47 am

Thank you for the compliments. The paint in the border pieces are a R&G transparent, I forget which number. The white glass in the border is float, blasted all over the back after all firing is complete. It does pop out pretty well, but we regret not going the extra step and using colorless antique glass or colorless float for the border. When you sandblast those glasses they scatter the light even better to an more intense white. Another thing is that the enamel is intense because it is applied very heavily with screen print. I've been doing this for a few years and haven't had any problems with it, but I bet it would be more durable if it was printed on a glass with a COE closer to that for which the enamel is designed. If this were to be an exterior glazing piece, I'd be worried about the paint crazing over time. My point is, that if you want to use enamels on clear glass like this, consider finding a colorless glass or white glass that has a higher COE.

Buttercup
Posts: 585
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: glass I'm working on

Postby Buttercup » Tue Feb 27, 2018 6:21 pm

Thank you very much for clarifying that, Don, and the advice regarding antique v float. Those borders have the sparkle and intensity of flashed glass.

Andrea R
Posts: 61
Joined: Fri Sep 30, 2005 10:52 am
Location: Canada

Re: glass I'm working on

Postby Andrea R » Wed Apr 04, 2018 8:24 pm

Alway perfect !!

Lucky the person that gets to look at that all day :)
Image
"C'est Moi (Its Me)"

Ed Cantarella
Posts: 155
Joined: Mon Feb 26, 2018 3:49 pm
Location: Highland, Michigan, USA

Re: glass I'm working on

Postby Ed Cantarella » Thu Apr 05, 2018 3:52 pm

WOW - really nice work Don. Some old-school stained glass people would want to string you up for mixing in fused elements,etc. "Consorting with the enemy" :lol:
HER last words were, "I'm melting, melting . . . " Dissenting opinions generally welcome for comic relief or personal edification. Sometimes both.

Don Burt
Posts: 559
Joined: Sun Mar 09, 2003 8:45 pm
Location: Cincinnati, Ohio
Contact:

Re: glass I'm working on

Postby Don Burt » Mon Oct 01, 2018 11:04 pm

Here's a piece I finished last month. It has pink striker petals fused onto the substrate, and glass paint for the rest of the imagery. The dark area at the bottom depicts Horsetooth Mountain ridge in Fort Collins.
Image

Havi
Posts: 603
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Re: glass I'm working on

Postby Havi » Tue Oct 02, 2018 12:30 am

VERY NICE!
Composition, technicalities
Beautiful,
Good for you

Havi
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com


Post Reply

Return to “Photos and Stuff”

Who is online

Users browsing this forum: No registered users and 6 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com