Playing with drop vases
Moderator: Brad Walker
-
Ed Cantarella
- Posts: 155
- Joined: Mon Feb 26, 2018 3:49 pm
- Location: Highland, Michigan, USA
Playing with drop vases
All are 10"+
HER last words were, "I'm melting, melting . . . " Dissenting opinions generally welcome for comic relief or personal edification. Sometimes both.
-
Ed Cantarella
- Posts: 155
- Joined: Mon Feb 26, 2018 3:49 pm
- Location: Highland, Michigan, USA
Re: Playing with drop vases
Ok, last one. For now. Have 6 others waiting to be beheaded
.
HER last words were, "I'm melting, melting . . . " Dissenting opinions generally welcome for comic relief or personal edification. Sometimes both.
-
Kevin Midgley
- Posts: 774
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada
Re: Playing with drop vases
Nice work Ed,
The tops don't have to be cut off if you drop the vase onto a nice wide base and fuse them together all at the same time.
Takes making a few duds to get it all perfectly done.
And all you thought you had to do was perfect the timing and temperature of the drop?
Don't forget the vase will not then go back through the ring so escape planning is required.
The tops don't have to be cut off if you drop the vase onto a nice wide base and fuse them together all at the same time.
Takes making a few duds to get it all perfectly done.
And all you thought you had to do was perfect the timing and temperature of the drop?
Don't forget the vase will not then go back through the ring so escape planning is required.
-
Ed Cantarella
- Posts: 155
- Joined: Mon Feb 26, 2018 3:49 pm
- Location: Highland, Michigan, USA
Re: Playing with drop vases
Thanks Kevin. Yeah, some we keep the tops on, others cut off. We like breaking, re-arranging and remelting the cut off pieces to make very similar sibling pieces or sets. I've made a few using an escape plan. And a few that couldn't escape - good-bye dear ring. 
HER last words were, "I'm melting, melting . . . " Dissenting opinions generally welcome for comic relief or personal edification. Sometimes both.