Hello friends

I am trying to carve hardnered fiber board and vermiculite to use for glass casting.
Are these the proper material to do this ?

What are best suggested separator to use with them?

thanks in advace for support and collaboration

mike from italy
thanks for sharing !

mike from italy


"secret of success?... passion & experience"

http://www.picturetrail.com/mikefromitaly
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: glass castings into molds

Post by Kevin Midgley »

For kiln casting use kiln wash.
For Dripping glass into the mold? .....maybe use kiln wash?

Vermiculite will need to have a good coat of kiln wash or it may show as unwanted patterns or texture in your glass piece.
Good luck and show us your results.
mikefromitaly
Posts: 67
Joined: Thu Apr 03, 2003 7:47 am
Location: italy-sicily
Contact:

Re: glass castings into molds

Post by mikefromitaly »

Thank you

What is best separator to get "shine" glass? is it also possible BN both on vermiculite or board?

thanks

mike
thanks for sharing !

mike from italy


"secret of success?... passion & experience"

http://www.picturetrail.com/mikefromitaly
Post Reply