Studio set up for plaster silica

Postby Rachel K » Tue Feb 03, 2015 5:35 am

Do you use a separate room for mixing plaster silica? I'm concerned about the plume of dust created when it is scooped and mixed? What are your solutions? What is acceptable ventilation? Yes I always wear my respirator! I am just worried about being in my studio working after mixing and cleanup has taken place.
Thank you

Greg Rawls
Posts: 147
Joined: Sun Mar 09, 2003 8:11 pm
Location: Charleston, SC
Contact:

Re: Studio set up for plaster silica

Postby Greg Rawls » Tue Feb 03, 2015 9:34 am

Rachel K wrote:Do you use a separate room for mixing plaster silica? I'm concerned about the plume of dust created when it is scooped and mixed? What are your solutions? What is acceptable ventilation? Yes I always wear my respirator! I am just worried about being in my studio working after mixing and cleanup has taken place.
Thank you


I would do the mixing outside so there is not an issue. Make sure it is not windy and still wear a P95 respirator that fits well.
Greg

Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Studio set up for plaster silica

Postby Bert Weiss » Tue Feb 03, 2015 11:57 am

The other big issue is keeping plaster out of your drain system. You don't want it in your pipes.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions

Rachel K
Posts: 6
Joined: Sun Dec 29, 2013 8:01 pm

Re: Studio set up for plaster silica

Postby Rachel K » Tue Feb 03, 2015 8:29 pm

Thank you for your posts. I use a Gelco sediment trap and it is wonderful.
Let me elaborate on my studio situation. I work in a converted car dealership. My section has 10 artists in separate rooms with 12 foot walls. The ceilings are 25 ft and we do not have windows. I am considering putting in an exhaust fan with a hood or another possibility is a down draft table. Water is not available in many places in the building but my studio has a sink. I could go out into the drive way but it makes clean up difficult ( no water) and I would be subjecting other artists to the silica. How dangerous is it to work where the dust has settled. Is it a heavy a particle is it? Will it become airborne every time I open my door?
I clean all my surfaces when I am done but it seams like there is always a residue.
Thanks again for your input


Post Reply

Return to “Kiln Casting”

Who is online

Users browsing this forum: No registered users and 7 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com