Postby raphy » Fri Jun 23, 2017 5:10 pm

Hello, I bought a murrini mold from Delphi, it has six shallow troughs about 6 in long which I want to fill with stringers and or frit, however I suppose a kiln cast schedule may work but as it is not very deep I am not sure what firing schedule to use. Has anyone ever used this mold. http://www.delphiglass.com/search?searc ... ini%20mold. it is the $21 one.
Thank you for any advice,