josie
Posts: 19
Joined: Fri Mar 14, 2003 1:41 pm
Location: Santa Fe

Wax in Steamer

Postby josie » Mon Oct 16, 2017 6:35 pm

I've never had this problem before. I used my Power Steamer 705 wallpaper steamer to remove wax from molds I made. As I cleaned up I thought the steamer tank felt heavy. Somehow some wax migrated into the water tank. Any ideas as to how to get it out?