What to do when tempered glass is not tempered? The glass in the salon door of a new yacht I am working on has a crack across one corner. We buy only tempered glass for these boats. There is an etched tempered stamp on this piece of glass. Obviously the glass was not tempered even though we payed extra for that. Anybody know about the legalities involved in this? Arrgh and this boat is supposed to be delivered Monday. R.
artist, owner of wanchese art studio, marine finisher

rosanna gusler
Posts: 730
Joined: Mon Mar 10, 2003 2:22 pm
Location: wanchese north carolina
Contact:

Re: faux tempered glass

Postby rosanna gusler » Wed Aug 13, 2014 11:01 am

Ñevermind. Re read the etched label. Safety not tempered. R.
artist, owner of wanchese art studio, marine finisher

Tony Smith
Posts: 1037
Joined: Sun Mar 09, 2003 5:59 pm
Location: Massachusetts, USA
Contact:

Re: faux tempered glass

Postby Tony Smith » Wed Aug 13, 2014 1:48 pm

At least safety glass will be easy to replace.

Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun


Post Reply

Return to “Business Topics”

Who is online

Users browsing this forum: No registered users and 9 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com

cron