I hate paying $45 for a replacement mullite rod - the ones that suspend my kiln elements. Does anyone have any thoughts about repairing them? They're hollow (and so even more doggone fragile). Thanks!
			
			
									
						
							"Every artist was first an amateur." 
--Ralph Waldo Emerson
			
						--Ralph Waldo Emerson
- 
				Kevin Midgley
 - Posts: 773
 - Joined: Mon Mar 10, 2003 11:36 am
 - Location: Tofino, British Columbia, Canada
 
Re: repairing mullite rods
borosilicate rod in the hollow tube?
			
			
									
						
										
						Re: repairing mullite rods
I don't know if this will help, but you can use hollow quartz glass rods instead, placing the coil inside the rod. It's cheaper and more efficient.
			
			
									
						
										
						Re: repairing mullite rods
That usually means replacing the entire system.  You can try heating the bent parts of the elements with a torch to straighten them out and then insert them into the quartz tubing but I'd start by spending the $45 (or find another supplier).
			
			
									
						
										
						- 
				Bert Weiss
 - Posts: 2339
 - Joined: Tue Mar 11, 2003 12:06 am
 - Location: Chatham NH
 - Contact:
 
Re: repairing mullite rods
Bert 
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
			
						Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Re: repairing mullite rods
Great link Bert. This company is the ticket for all your kiln needs - I really like their very affordable stock coils for our home-made kilns!
			
			
									
						
										
						Re: repairing mullite rods
Mark- I've used them for 2 large homemade ones.  Great people to deal with.
			
			
									
						
										
						- 
				Bert Weiss
 - Posts: 2339
 - Joined: Tue Mar 11, 2003 12:06 am
 - Location: Chatham NH
 - Contact:
 
Re: repairing mullite rods
They can make any element for any kiln, on a custom basis. I heartily endorse them.Mark Hall wrote:Great link Bert. This company is the ticket for all your kiln needs - I really like their very affordable stock coils for our home-made kilns!
Bert 
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
			
						Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions