Page 1 of 1
					
				Glass Casting Forum ?
				Posted: Fri Feb 20, 2015 1:50 pm
				by Glenn
				Is there a forum that is specifically geared towards glass casting?  This is a great forum, but seems mostly for fusing & slumping thinner glass.  Craftweb is mostly folks that make blown glass.
I'm just curious if there is a forum where more glass casters hang out.
			 
			
					
				Re: Glass Casting Forum ?
				Posted: Thu Feb 26, 2015 7:38 pm
				by Joe Pfeifer
				This is it!
Take some time to look through the older postings. There are some very knowledgeable artists that contribute here. As you get involved we hope you will also contribute. Ask questions on what you are working on. There are experienced kiln builders, and people with all of the formulas, and schedules you will need.
			 
			
					
				Re: Glass Casting Forum ?
				Posted: Thu Feb 26, 2015 8:42 pm
				by Kevin Midgley
				from a post I made in april 2013:
Re: Archive posts
Yeah and the one series of posts I miss Brad are those of 
glassburl, Hugh Mckay and his glass casting processes.
He's doing fine work now:
http://www.castglassforms.com/index.html
That ought to inspire the newbees.