Post by cindabr »

:D Thanks everyone for answering my other post..now I have another question.

I've been using strickly either Spectrum 96 fusible or Bullseye fusible. I know NOT to mix the two. But can Wasser fusible (90 COE) be used with Bullseye?

So can you use other manufacturers of glass with together as long as the COE's are the same?

Thanks
Cinda
dee
Posts: 302
Joined: Tue Mar 11, 2003 5:20 pm
Location: Atlanta GA
Contact:

Re: COE's

Post by dee »

cindabr wrote::D Thanks everyone for answering my other post..now I have another question.

I've been using strickly either Spectrum 96 fusible or Bullseye fusible. I know NOT to mix the two. But can Wasser fusible (90 COE) be used with Bullseye?

So can you use other manufacturers of glass with together as long as the COE's are the same?

Thanks
Cinda
cinda, the coe is usually the important thing - i have both be and uroboros 90 coe and they go together just fine - wasser tho might reach full fuse at different temperatures, check dti's website for technical information on that. it may just take a bit of experimentation on your part to find the happy fusing temp of a combo of be and wasser....
Dee Janssen
Unicorn's Creations Studio
http://ucjewelry.com
dee@ucjewelry.com
Amy Schleif-Mohr
Posts: 280
Joined: Sun Mar 09, 2003 5:18 pm
Location: Milwaukee

Post by Amy Schleif-Mohr »

Sort of, you should always test first if you are going to use more than one manufacturer.

Amy
Lisa Allen
Posts: 212
Joined: Sun Mar 09, 2003 3:23 pm
Location: Memphis, TN
Contact:

Post by Lisa Allen »

Amy Schleif-Mohr wrote:Sort of, you should always test first if you are going to use more than one manufacturer.

Amy
I agree with Amy. I had some Uroboros 90 (opaque yellow) that I used with BE and there was lots of stress in the finished piece, even tho they were both 90 and should have been compatible. Now I always test first.