Blasting Resist in a Pinch?
I need to do some fairly deep sand blasting this weekend -- but don't have any "real" resist. It seems the only way to buy the stuff is to mail order it -- which probably precludes me having it in time.
Any suggestions on decent alternatives. For this project I don't need (and in fact don't want) crisp lines.
Thanks,
Paul
Any suggestions on decent alternatives. For this project I don't need (and in fact don't want) crisp lines.
Thanks,
Paul
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
You can paint on elmers glue or asphaltum or liquid latex (the stuff used for coating tool handles)Bob wrote:Hey Paul,
What about "MacTac" shelve covering. It comes in clear. Or duct tape/masking tape.
Cheers,
Bob
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
-
Nancy Juhasz
- Posts: 113
- Joined: Sun Mar 09, 2003 10:10 pm
- Location: Ohio
-
Nikki ONeill
- Posts: 169
- Joined: Mon Mar 10, 2003 11:55 am
- Location: Silver Spring, MD
- Contact:
It just rubs right off. These "liquid resists" such as spray adhesive, contact cement, and rubber cement are for texture. You aren't going to be doing any straight lines, or cutting when using them. They're primarily used to texture an already sandblasted area. Normally, you would resist your blank, bowl, 4' by 6' panel of float, lay out your design, cut, peel, and blast. Then, you would go back into selected areas with a liquid resist. These coatings can be manipulated, and when used in conjunction with sandblasting and acid etching can make an extremely interesting textured effect. I believe Markian Olynyk of Vancouver was the first to discover this. He was certainly the first one using them here. many years a go. He can make amazing effects with this process and paint. Elaborate, multi-panel screens. Brocklohman wrote:Does the contact cement peel off or do you have to use a solvent?
My memory is so good, I can't remember the last time I forgot something . . .
-
David Cutler
- Posts: 2
- Joined: Wed Jun 18, 2003 12:36 am
- Location: Mosier, Oregon
Maybe you should look at sign supply houses for the resist if there is one near you. The one I use stocks it regularly. Also you might try sign makers that specialize in wood sandcarved signs or monument makers in your town. They may sell you what you need if it is not much until your resist comes in.