long strip of ruby glass

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Tom Fuhrman
Posts: 187
Joined: Mon Mar 10, 2003 11:44 am
Location: eastern Tennessee
Contact:

long strip of ruby glass

Post by Tom Fuhrman »

I am in need of a piece of transparent ruby glass that is 80" X 14". does anyone know of anybody that could supply this? I know Spectrum could probably do it, but not sure if they would. This is a replacement for a church window and must match the others that are this size (one piece) that are housed between two pieces as an insulated unit. Any ieas or leads on where to procure this "animal"? Tenn. Tom http://www.fuhrmanglass.com
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: long strip of ruby glass

Post by Bert Weiss »

Fuhrman Glass Studios Inc wrote:I am in need of a piece of transparent ruby glass that is 80" X 14". does anyone know of anybody that could supply this? I know Spectrum could probably do it, but not sure if they would. This is a replacement for a church window and must match the others that are this size (one piece) that are housed between two pieces as an insulated unit. Any ieas or leads on where to procure this "animal"? Tenn. Tom http://www.fuhrmanglass.com
Tom

I think that Wissmach's full sheet size is 84" long. If it is old, chances are that it is Wissmach.

As I said in the tempered glass thread. It is possible to laminate 2 pieces of colored glass on to 1 piece of tempered or annealed glass if no real match can be found.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
David Williams

Re: long strip of ruby glass

Post by David Williams »

Fuhrman Glass Studios Inc wrote:I am in need of a piece of transparent ruby glass that is 80" X 14". does anyone know of anybody that could supply this? I know Spectrum could probably do it, but not sure if they would. This is a replacement for a church window and must match the others that are this size (one piece) that are housed between two pieces as an insulated unit. Any ieas or leads on where to procure this "animal"? Tenn. Tom http://www.fuhrmanglass.com
The problem you're going o find is getting someone to melt a whole tank for you when you only want one piece. There's no way Spectrum or any other sheet glass maker would do that. If you really need a custom color sheet glass I think the most likely way is to commision a mouthblown sheet. They can get very close with applied color rather than having to figure out a color melt that will match what you want. In fact a good part of mouthblown glass business is church restoration and such. They do call it antique afterall. The only problem is that any mouthblown sheet will fall way short of 80"
Mike Byers
Posts: 56
Joined: Mon Mar 10, 2003 6:57 pm
Location: west central Indiana
Contact:

Post by Mike Byers »

Check with Kokomo; I recall seeing some very large sheets at their factory.
Marty
Posts: 865
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Post by Marty »

For David- Spectrum produces a continuous ribbon of glass- it's not cut until it reaches the cool end of the lehr. Theoretically they could custom-cut at that end.
Marty
Brian and Jenny Blanthorn
Posts: 353
Joined: Mon Mar 10, 2003 5:25 pm
Location: UK
Contact:

Re: long strip of ruby glass

Post by Brian and Jenny Blanthorn »

Fuhrman Glass Studios Inc wrote:I am in need of a piece of transparent ruby glass that is 80" X 14". does anyone know of anybody that could supply this? I know Spectrum could probably do it, but not sure if they would. This is a replacement for a church window and must match the others that are this size (one piece) that are housed between two pieces as an insulated unit. Any ieas or leads on where to procure this "animal"? Tenn. Tom http://www.fuhrmanglass.com
I think U got a few problems

Colour match n then if U do find a big peice of glass transporting it

Then putting it in

U might try a Q over a stainded glass type BB
Image
charlie
Posts: 961
Joined: Mon Mar 10, 2003 3:08 pm

Re: long strip of ruby glass

Post by charlie »

Fuhrman Glass Studios Inc wrote:I am in need of a piece of transparent ruby glass that is 80" X 14". does anyone know of anybody that could supply this? I know Spectrum could probably do it, but not sure if they would. This is a replacement for a church window and must match the others that are this size (one piece) that are housed between two pieces as an insulated unit. Any ieas or leads on where to procure this "animal"? Tenn. Tom http://www.fuhrmanglass.com
can't you fuse one up? just find someone with an 82" length kiln.

you could ask on the stained glass email list at glass@bungi.com. you might have to join it first at glass-request@bungi.com though.
David Williams

Post by David Williams »

Marty wrote:For David- Spectrum produces a continuous ribbon of glass- it's not cut until it reaches the cool end of the lehr. Theoretically they could custom-cut at that end.
Marty
Sure I'm aware of that. Its not as big a deal if he just wants a longer sheet of a stock color if the equipment can be set up to do that. And, Spectrum does make a pretty nice ruby. The problem is if Tom needs to match up a particular ruby.

Ps. Sorry, I guess I didn't read his post well. He didn't say anything about a custom color, I stand corrected. If any old ruby will do I'd give Jim Gregory at Spectrum a call and try and work something out. They probably only make that ruby once a year though so you may be in for a wait Tom.
Tom Fuhrman
Posts: 187
Joined: Mon Mar 10, 2003 11:44 am
Location: eastern Tennessee
Contact:

Post by Tom Fuhrman »

Thanks for all the suggestions. For everyones info, Kokomo Glass had it, they make 32" X 84" sheets. Tenn. Tom
Post Reply