need a supplier for Fiberboard kiln shelves.

Post by Michael McNerney »

Can anyone suggest a supplier close to ohio that sells these wholesale?
Need a shelf thats about 28 X 58

Thank you in advbance
Michael
Ron Coleman
Posts: 468
Joined: Sun Mar 09, 2003 3:20 pm
Location: Columbus, Ohio USA

Post by Ron Coleman »

A local source for fiber and ifb.

Out past the airport, off Taylor Station Rd.

Adrian L Wallick Co
614-863-1868
1013 Gahanna Pkwy
ReynoldsburgOH 43068

Ron
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: need a supplier for Fiberboard kiln shelves.

Post by Bert Weiss »

Michael McNerney wrote:Can anyone suggest a supplier close to ohio that sells these wholesale?
Need a shelf thats about 28 X 58

Thank you in advbance
Michael
I don't know of an off the shelf board that works and comes 58". Unifrax standard sizes go up to 42" x 48". You can order a 9' sheet from Unifrax but you will have to pay crating and shipping from Niagra Falls. They are pricey.

Don't fall for the Marinite. It sucks.

My solution is 2 pieces of board covered with one piece of blanket and then powder the blanket. If you want a surface with less texture, paper will also work. It is less durable.

If you find a board that meets your needs, let us know about it.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Michael McNerney
Posts: 41
Joined: Tue Mar 18, 2003 12:22 pm
Location: Hilliard, Ohio

Post by Michael McNerney »

Thankx

Mr. Coleman
I met your neighbor at the worthington arts festival last weekend.
I gave her one of my business cards and told her to stick it in your screen door. Thought you might get a kick out of it.




,and Thank you Bert
I will let everyone know what I find out.