Post by lohman »

Actually I had UV adhesives in mind but if I don't have to grind the back surface using a more viscous resin--Hey, I can get with that.
But, doesn't the rounded fired edge of the glass pieces create an undercut and make cleaning difficult? Is there enough ooze of resin that can be trimmed with an Exacto blade held perpendicular to the base glass leaving the undercut filled with resin?