Pocelain disk ????
Moderators: Brad Walker, Tony Smith
-
- Posts: 32
- Joined: Sun Mar 09, 2003 6:18 pm
- Location: Virginia, USA
- Contact:
Pocelain disk ????
hello everyone. does anyone know if i can fuse on porcelain disks and the glass will stick to it. I dont want it to come off. trying to make some small mosiac pieces to wear as jewelery. Maybe putting a clear glass over the top of it. Just a thought. Alice
-
- Posts: 86
- Joined: Sun Mar 09, 2003 6:21 pm
- Location: Cheshire. Oregon
- Contact:
-
- Posts: 382
- Joined: Sun Mar 09, 2003 8:10 pm
- Location: Washington DC Metropolitan Area
- Contact:
-
- Posts: 32
- Joined: Sun Mar 09, 2003 6:18 pm
- Location: Virginia, USA
- Contact:
porcelain disk THANKS
I am going to try it. Hey as long as it dont damage my kiln i will go for it.
As a matter of fact I am going to try doing it tomorrow!!! Thanks for the information. But I do have another question.... can i lay the porcelain disk on the kiln wash shelf just incase the glass does spill over??? will doing this hurt the porcelain disk??? thannnnnnnnkkkkkkkksssssss again you fine people!!!! Alice
As a matter of fact I am going to try doing it tomorrow!!! Thanks for the information. But I do have another question.... can i lay the porcelain disk on the kiln wash shelf just incase the glass does spill over??? will doing this hurt the porcelain disk??? thannnnnnnnkkkkkkkksssssss again you fine people!!!! Alice
-
- Posts: 32
- Joined: Sun Mar 09, 2003 6:18 pm
- Location: Virginia, USA
- Contact:
Porcelain Disk Test
Well I did my test on the little disks. One I put dichoric on and capped. So far it looks great no cracks on that one. I guess that is because I used little pieces and capped with clear glass. The second one I put some copper bits on porcelain and then put the clear glass on that. I was able to pull that apart but a coating of the porcelain stay on the back. Now this one cracked. Not the porcelain but the glass. Just a crackle look. Still in one piece. The mad scientist is heading back to the lab for more creating
Thanks Alice
Thanks Alice