glass thickness ?
Moderators: Brad Walker, Tony Smith
glass thickness ?
I am new to fusing and am learning much as each firing comes out. From what I have read on this board and other info, glass is going to go to 1/4 in thickness if fired to full fuse and over. my question is what temp over full fuse or what flux can be applied to the glass to allow it to flow back to a thinner form.
Will this break down the glass and cause it to shatter on cooling.
I am getting very interesting pieces with 3 layers of wasser and a dichroic chip fired to 1400, but its too thick for earings. I am hoping to get the glass to flow thinner.
Thanks all for this forum, this is one of the best tech forums around on any subject wyndham@ac.net
Will this break down the glass and cause it to shatter on cooling.
I am getting very interesting pieces with 3 layers of wasser and a dichroic chip fired to 1400, but its too thick for earings. I am hoping to get the glass to flow thinner.
Thanks all for this forum, this is one of the best tech forums around on any subject wyndham@ac.net
-
Brad Walker
- Site Admin
- Posts: 1542
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
By tack fusing and keeping the temperature below 1400, you're already keeping the glass from getting heated enough to flow to 1/4 inch thickness. If you heat it higher, then it will try its best to reach an equilibrium thickness of around 1/4 inch. (This is a law of physics, like gravity. Just as you can't reverse gravity, there is no "flux" that you can add to get the glass to "flow thinner".)
I can only think of two ways to trick the process and get a piece to be thinner and then remain at that thickness as it cools. The first is to to manipulate it when hot by rolling or a similar method (for instance, sheets are rolled when hot, then quickly cooled). The second is to use coldworking equipment (usually a reciprolap) to grind the piece thin after firing. That's labor intensive, but you can reach 1/16" or thinner.
I can only think of two ways to trick the process and get a piece to be thinner and then remain at that thickness as it cools. The first is to to manipulate it when hot by rolling or a similar method (for instance, sheets are rolled when hot, then quickly cooled). The second is to use coldworking equipment (usually a reciprolap) to grind the piece thin after firing. That's labor intensive, but you can reach 1/16" or thinner.
-
Phil Hoppes
- Posts: 298
- Joined: Wed Mar 12, 2003 2:20 pm
- Location: Overgaard, AZ
Many have put it to me that glass "wants" to be 6mm or 1/4 inch thick. The scientific explaination is not that it "wants" to be but the surface tension of the material when it is in a liquid form forces it to be this thickness. This surface tension is a function of many things, many of which I don't know but among them I have to believe is the density of the material and the viscosity of the material. Short of molecular engineering or changing the gravitational constant of the earth, you can't do much about the density of the material, but you might be able to affect the viscosity by some type of surface flux as you mention. I'm not aware of any that will do this unfortunately. I know that BE sells 1.5mm clear but I believe that they achieve this by mechanically rolling the glass to that thickness and cooling it before it has a chance to flow back to a thicker state, which is essentially what they do with the 3mm that is their stock in trade. Maybe someone one else on the board here has some experience in this area, although I've not heard of it.
Phil
Phil
it's called a surfactant. the hard part would be to find one that's stable at 1500F and won't affect other glass properties, like color for instance.Phil Hoppes wrote:Many have put it to me that glass "wants" to be 6mm or 1/4 inch thick. The scientific explaination is not that it "wants" to be but the surface tension of the material when it is in a liquid form forces it to be this thickness. This surface tension is a function of many things, many of which I don't know but among them I have to believe is the density of the material and the viscosity of the material. Short of molecular engineering or changing the gravitational constant of the earth, you can't do much about the density of the material, but you might be able to affect the viscosity by some type of surface flux as you mention. I'm not aware of any that will do this unfortunately. I know that BE sells 1.5mm clear but I believe that they achieve this by mechanically rolling the glass to that thickness and cooling it before it has a chance to flow back to a thicker state, which is essentially what they do with the 3mm that is their stock in trade. Maybe someone one else on the board here has some experience in this area, although I've not heard of it.
Phil
-
Paul Tarlow
- Posts: 344
- Joined: Sun Mar 09, 2003 4:06 pm
- Location: Helios Kiln Glass Studio - Austin
- Contact:
There was a thread some time ago about "squeezing" glass thinner by putting a second kiln shelf (possible with weights on top) on top of the fusing and having spacers between the two shelves to set the final width.
There was broad disagreement about if it would work or not.
Its on my (very long) list of experiments I want to try. I don't know if anyone ever gave it a shot.
- Paul
There was broad disagreement about if it would work or not.
Its on my (very long) list of experiments I want to try. I don't know if anyone ever gave it a shot.
- Paul
-
Lani McGregor
- Posts: 121
- Joined: Mon Mar 10, 2003 2:12 pm
- Location: Portland, OR
- Contact:
Paul,Paul Tarlow wrote:There was a thread some time ago about "squeezing" glass thinner by putting a second kiln shelf (possible with weights on top) on top of the fusing and having spacers between the two shelves to set the final width.
There was broad disagreement about if it would work or not.
Its on my (very long) list of experiments I want to try. I don't know if anyone ever gave it a shot.
- Paul
Before BE ever made its thin glass (1991?) there was a guy (in Washington state, I think) who sent me lots of pretty impressive slides of work done using home-made thin sheets of BE that he said was made this way – heating and pressing 1/8 inch glass between shelves in a kiln. We never tried it, but the slide evidence of his own success with the process seemed valid.
Wish I could remember his name…. and now I’m thinking that it might have been Corvallis, OR and not WA…. sorry…. it’s been 15 years or more…(I know the name will come to me at 3 am…. can I call you?)
-Lani
-
Lani McGregor
- Posts: 121
- Joined: Mon Mar 10, 2003 2:12 pm
- Location: Portland, OR
- Contact:
thanks for the input
Well, this is kinda what I was thinking might be the case, gravity works. Thanks for the input. Would putting a weight on top of a piece be a problem when the glass cools at 960 quarts inversion? I'll try with a broken piece of kiln shelf and post later. Thanks wyndham@ac.net
-
Paul Tarlow
- Posts: 344
- Joined: Sun Mar 09, 2003 4:06 pm
- Location: Helios Kiln Glass Studio - Austin
- Contact:
-
Lani McGregor
- Posts: 121
- Joined: Mon Mar 10, 2003 2:12 pm
- Location: Portland, OR
- Contact: