In this firing I went up 300 dph to 1000, soak 5, 500 dph 1250, soak 5, afap to 1425, soak 10, afap to 960, soak 45, 100 dph to 700, off.
On the way up one of the tiles broke in a classic s shaped curve. The edges of the break are nicely rounded.
Would this indicate that my tiles had not been properly annealed prior to this fusing? The fact that only one broke puzzles me. I would expect that if one was stressed, all should have been stressed.
(and doesn't this crap always happen when you are trying to finish up a delivery????)
![Evil or Very Mad :evil:](./images/smilies/icon_evil.gif)
Thanks for any and all comments.
Barbara