I saw in the archive several different mixes for kiln wash, is the mixture
according to weight  or volume?
			
			
									
						
										
						Kiln wash mix
Moderators: Brad Walker, Tony Smith
- 
				Bert Weiss
 - Posts: 2339
 - Joined: Tue Mar 11, 2003 12:06 am
 - Location: Chatham NH
 - Contact:
 
Re: Kiln wash mix
The recipes that I know are by weight. 50/50 or 80% alumina/20% EPKBruce wrote:I saw in the archive several different mixes for kiln wash, is the mixture
according to weight or volume?
There is probably a pretty big difference between weight and volume. On the other hand if both of those formulas work it isn't rocket science.
Bert 
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
			
						Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Re: Kiln wash mix
Yeah, think of it as a water based paint. You can thin it all you like, but you still have to put enough coats on to properly prepare the shelf. It's the solids left, after the water is gone, that you're concerned about. A quick rule of thumb for firing 90 and 96 glasses on mullite, is that you should not be able to see any of the colour of the kiln shelf through your coating. I apply 8 to 12 coats of relatively thin kiln wash to achieve this. BrockBert Weiss wrote:The recipes that I know are by weight. 50/50 or 80% alumina/20% EPKBruce wrote:I saw in the archive several different mixes for kiln wash, is the mixture
according to weight or volume?
There is probably a pretty big difference between weight and volume. On the other hand if both of those formulas work it isn't rocket science.
My memory is so good, I can't remember the last time I forgot something . . .