decorating slumped bottles

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
SueW
Posts: 3
Joined: Sat Apr 26, 2003 12:58 pm
Location: Nanaimo BC

decorating slumped bottles

Post by SueW »

I finally have mastered the slumping of bottles with wire staying in and nict edges, I now wonder if anyone has tried putting stuff inside the bottle. If so what did you use. I etched grapes and vines on the back of my bottles and they look great.
Diane
Posts: 56
Joined: Sun Mar 09, 2003 3:59 pm
Location: Kennebunkport, Maine

Post by Diane »

I've done alot of bottles but have never had any success actually putting anything inside them . You would be faced with alot of compatibility problems I'm affraid. I've painted on them or glued the original labels back on though.
Now that you've mastered bottles..on to bigger and more challenging things
Good Luck
Diane