i blasted a pattern into irid. i'm going to fire the glass irid side up, and would like to coat the top to prevent devit. i know i can use spray-a, but would like to have a lead free surface. i've used borax, but not over irid. does it work out ok, or does it make irid be blotchy?
anyone have experience using borax over b.e. irid?
thanks
borax over irid
Moderators: Brad Walker, Tony Smith
-
Tony Serviente
- Posts: 328
- Joined: Thu May 29, 2003 11:48 am
- Location: Ithaca,NY
- Contact:
-
Phil Hoppes
- Posts: 298
- Joined: Wed Mar 12, 2003 2:20 pm
- Location: Overgaard, AZ
-
paulfjackson
- Posts: 9
- Joined: Thu Jul 10, 2003 10:12 am
- Location: Grand Rapids, Michigan
Borax over Irid
I coated a piece of Green Irid last night before slumping at 1300. No body was there to tell me not to. Turned out nice and shiney, especially the edge.
Paul F. Jackson
Looking Glass Studio
"What are you looking at?"
Looking Glass Studio
"What are you looking at?"
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Borax over Irid
Coated with what?paulfjackson wrote:I coated a piece of Green Irid last night before slumping at 1300. No body was there to tell me not to. Turned out nice and shiney, especially the edge.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
paulfjackson
- Posts: 9
- Joined: Thu Jul 10, 2003 10:12 am
- Location: Grand Rapids, Michigan