Another question about big bubbles
Moderators: Brad Walker, Tony Smith
-
Jackie Braitman
- Posts: 27
- Joined: Mon Jul 28, 2003 9:53 am
- Location: Takoma Park, MD
- Contact:
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Another question about big bubbles
[quote="Jackie in Washington DC"]I’m having problems with big (2 ½â€
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
Jackie Braitman
- Posts: 27
- Joined: Mon Jul 28, 2003 9:53 am
- Location: Takoma Park, MD
- Contact:
bubble
Have you ever check to see when the bubble started to form. I usually go from 1100 to 1280 at 60dph and then sit and soak for 25 min. I then only ramp at about 400 to final temp. I have found this has worked with all my pieces and I have not come up with no devit or and bubbles. This firing schedule I use with float spectrum and BE. This has solved all my bubbles problems. But if your shelf is not flat it probably won't matter. You possibly might get away with some thick fiber paper if its just a little off. If you put the shelf on a table you can squat down and put a straight edge across shelf in 2 or 3 places and look for light between the shelf and the straight edge. Tom
I did 2 things. I was firing Spectrum and only 1 layer. I used 2 segments (as you have described) to get to full fuse temp, but I ramped at 300 for both segments. That worked for me. The next time I fired a similar piece, I used the same schedule, but I also put 1/8 inch fiber under the 1/16 paper as someone had suggested. It worked as well. So, unfortunately, now I don't really know which of the 2 is giving me the good results
. I will probably try again without the 1/8 inch paper, but I sure do hate the thought of opening to find a big bubble.
I have some new paper and I'm scared to death to use it!
I have some new paper and I'm scared to death to use it!
-
Jackie Braitman
- Posts: 27
- Joined: Mon Jul 28, 2003 9:53 am
- Location: Takoma Park, MD
- Contact:
Tom, Ross - Thanks.
Yeah - I've been in the dumps all day because the last bubble was in a piece that I need to deliver soon and I don't even have enough replacement glass.
I'll check the shelf for level -- I'm suspecting Bert is right because at least two of the holes appeared at about the same place on the shelf.
If the shelf isn't perfectly level, will 1/8th inch fiber paper solve the problem? If so, I have enough of that until I can order a new shelf from Bullseye.
Yeah - I've been in the dumps all day because the last bubble was in a piece that I need to deliver soon and I don't even have enough replacement glass.
I'll check the shelf for level -- I'm suspecting Bert is right because at least two of the holes appeared at about the same place on the shelf.
If the shelf isn't perfectly level, will 1/8th inch fiber paper solve the problem? If so, I have enough of that until I can order a new shelf from Bullseye.
Jackie
-
Jackie Braitman
- Posts: 27
- Joined: Mon Jul 28, 2003 9:53 am
- Location: Takoma Park, MD
- Contact:
Yep - just checked the shelf and there are two very slight dips in the shelf (maybe 1/16' deep) in the two locations I've seen bubbles.
The last firing was on Thinfire and it didn't stop the bubbles. But I'll try two blanks using 1/8th" paper and see if that works -- while I'm waiting for a Bullseye shelf to come in.
Thanks for all the help.
The last firing was on Thinfire and it didn't stop the bubbles. But I'll try two blanks using 1/8th" paper and see if that works -- while I'm waiting for a Bullseye shelf to come in.
Thanks for all the help.
Jackie