hi all, can any of you float frit users share opinions on that product? problems, what you like, how is the confetti, info on how the various grain sizes behave, color saturation................other than that, not much. i am going to order some i think. rosanna
I have used cherry red, chrome green, and opaque blue in sizes 2 and 3 on 1/4" float, no experience with powder or confetti. Fired to 1500/1550 and got good results. I mixed with just enough clear fyre to hold the grains together and packed it into a stencil about 3/32" thick. The only problem I saw was some rough patches like devit in places on the chrome green only.
Best wishes,
Tom in Texas
Best wishes,
Tom in Texas
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
-
Judy Schnabel
- Posts: 195
- Joined: Mon Mar 10, 2003 9:45 pm
- Location: SW FL
- Contact: