a successful fuse

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
maggie may
Posts: 10
Joined: Sat Jul 12, 2003 6:05 pm
Location: Santa Fe

a successful fuse

Post by maggie may »

Hi,
I wanted to say thanks to Jerry and Kitty for their help with my
bubble problem. I did use fiber paper and had a perfectly
fused round piece. Jerry, I followed your firing schedule. Today
I am slumping the piece. I'm keeping my fingers crossed.
Thanks,
Marilyn
Jerry Barnett
Posts: 55
Joined: Wed Mar 12, 2003 11:40 am
Location: Texas, USA

Post by Jerry Barnett »

Glad the fuse worked, and hope the slump goes well. Jerry