Help!! I would like to reapply the label to the front of a wine bottle which has been slumped. Does anyone have any advice on how to do this? I am especially interested in finding something to "coat" the label with to make it food safe and durable enough to cut on.
Thanks-
Linda
FOOD SAFE DECORATING on Slumped Wine Bottles
Moderators: Brad Walker, Tony Smith
-
Katy Mattice
- Posts: 6
- Joined: Sun Mar 09, 2003 9:00 pm
- Location: Florida and Wisconsin
-
Mark Selleck
- Posts: 36
- Joined: Mon Mar 10, 2003 1:52 pm
- Location: Waxhaw, NC
- Contact:
durable wine bottle decoration
The only viable way to put something on the top surface of the bottle, that will resist cutting and be food safe, is to paint/screen print with a food safe paint that can be fired on, or to etch a design. I know of no workable way to put the original label on the top surface that will offer the durability you need for use as a serving platter.