making holes
Moderators: Brad Walker, Tony Smith
- 
				cheryl kumiski
 - Posts: 9
 - Joined: Fri Jul 18, 2003 1:55 pm
 - Location: chuluota, florida
 - Contact:
 
making holes
i was using 1/4" grinder bits to make holes in plates so they would accept clock works. the problem being 1 bit equals 3 holes. yikes!!! and i can't figure out how to use a drill press without electrocuting myself. my kingdom for a solution!!
			
			
									
						
										
						- 
				Barbara Muth
 - Posts: 382
 - Joined: Sun Mar 09, 2003 8:10 pm
 - Location: Washington DC Metropolitan Area
 - Contact:
 
- 
				starchimes (Andrea)
 - Posts: 26
 - Joined: Tue May 20, 2003 11:39 am
 - Location: Dallas, TX
 - Contact:
 
Try getting your bits at http://www.lopacki.com.  The prices are good.  Bits last a good while.    I can usually get about 50 holes per bit.
Regards,
Andrea
			
			
									
						
										
						Regards,
Andrea
- 
				paulajane
 
I purchased some bits that would not work with my flexible shaft set up. So we bought a cheap $20 drill press stand at Harbor Freight Tools and then adapted it to hold a cordless battery operated a drill. To keep it going steadily we slide a tie wrap over the button because battery operated drills do not have buttons to press to keep them going continuously. It works great.
Paula
			
			
									
						
										
						Paula
- 
				cheryl kumiski
 - Posts: 9
 - Joined: Fri Jul 18, 2003 1:55 pm
 - Location: chuluota, florida
 - Contact:
 
thanks paula--this seems the most effective. i did check the archives and most of the info concerns a dremel tool. since i need a 1/4" hole drilled through 6 layers of glass the dremel isn't an option. i'll try a regular drill with diamond bits.paulajane wrote:I purchased some bits that would not work with my flexible shaft set up. So we bought a cheap $20 drill press stand at Harbor Freight Tools and then adapted it to hold a cordless battery operated a drill. To keep it going steadily we slide a tie wrap over the button because battery operated drills do not have buttons to press to keep them going continuously. It works great.
Paula
cheryl
- 
				cheryl kumiski
 - Posts: 9
 - Joined: Fri Jul 18, 2003 1:55 pm
 - Location: chuluota, florida
 - Contact:
 
- 
				cheryl kumiski
 - Posts: 9
 - Joined: Fri Jul 18, 2003 1:55 pm
 - Location: chuluota, florida
 - Contact:
 
thank you!! will do.starchimes wrote:Try getting your bits at http://www.lopacki.com. The prices are good. Bits last a good while. I can usually get about 50 holes per bit.
Regards,
Andrea
cheryl
- 
				Dick Ditore
 - Posts: 58
 - Joined: Mon Mar 10, 2003 12:56 pm
 - Location: San Diego, Ca
 - Contact:
 
- 
				Paul Tarlow
 - Posts: 344
 - Joined: Sun Mar 09, 2003 4:06 pm
 - Location: Helios Kiln Glass Studio - Austin
 - Contact:
 
- 
				Alecia Helton
 - Posts: 108
 - Joined: Mon Aug 25, 2003 12:35 am
 - Location: outside of Dallas TX
 
Making holes
Sorry to be a late reply.  I just joined the list.
I bought my drill press at Home Depot, the drill was included with the press. I buy the hollow-core diamond bits from Rio Grande.
To drill with water: I place a large plastic lid on the base plate to protect the metal from from the wet sponge that lays on top of it. I use a squirt bottle to keep the drill and glass wet.
There are times when you really need three hands. And I have used my chin at times, but I've never feared electrocution.
Hope this helps.
 
Alecia
			
			
									
						
							I bought my drill press at Home Depot, the drill was included with the press. I buy the hollow-core diamond bits from Rio Grande.
To drill with water: I place a large plastic lid on the base plate to protect the metal from from the wet sponge that lays on top of it. I use a squirt bottle to keep the drill and glass wet.
There are times when you really need three hands. And I have used my chin at times, but I've never feared electrocution.
Hope this helps.
Alecia
Alecia Helton
Wear Original Wonders!
Carrollton TX
			
						Wear Original Wonders!
Carrollton TX