i remember seeing something where a guy has this pattern bar over a sharp edge, and then whacks the thing, and that breaks off a piece of the bar,,,,has anyone done this,,,,the specifics would be appreciated,,,im trying to find out a way of making slices, WITHOUT a saw,,,,,,can someone tell me how long it take to cut through a 1" sq pattern bar, with a saw, do you have to cut through the whole thing, or can you break it off, once you get going
thanks
rodney
PATTERN BAR,,,,,,BREAKING
Moderators: Brad Walker, Tony Smith
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: PATTERN BAR,,,,,,BREAKING
Rodneyrodney wrote:i remember seeing something where a guy has this pattern bar over a sharp edge, and then whacks the thing, and that breaks off a piece of the bar,,,,has anyone done this,,,,the specifics would be appreciated,,,im trying to find out a way of making slices, WITHOUT a saw,,,,,,can someone tell me how long it take to cut through a 1" sq pattern bar, with a saw, do you have to cut through the whole thing, or can you break it off, once you get going
thanks
rodney
Glass blowers use a carbide wedge and hammer to cut color bars. They don't need a clean shape though, just a hunk of glass. If you want to stack your pattern bars next to one another and fuse them, they need to be square and clean. A saw is the only way to do this. You can rent one from the tile dept at Home Depot for an hour and cut away.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
The blade needs to be wet or the temperature will quickly get to the point where it causes the glass to fracture. The blade either runs through a tub of water, or it has water pumped onto it... either way, you need coolant at the blade/glass contact point.
Tony
Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
Re: PATTERN BAR,,,,,,BREAKING
home depot will cut it for you at .25 per cut, or just find a tile guy and stop by with a 12 pack.Bert Weiss wrote:
Rodney
Glass blowers use a carbide wedge and hammer to cut color bars. They don't need a clean shape though, just a hunk of glass. If you want to stack your pattern bars next to one another and fuse them, they need to be square and clean. A saw is the only way to do this. You can rent one from the tile dept at Home Depot for an hour and cut away.