This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.
Moderators: Brad Walker , Tony Smith
Randy W
Posts: 91 Joined: Sun Mar 09, 2003 6:19 pm
Location: Racine, Wisconsin
Post
by Randy W » Thu Aug 28, 2003 4:11 pm
Even though it was square, the table slid a little diagonally. I fixed that by placing a very thin fiber washer between the table and the sliding bracket. The pencil is pointing at it.
Here is a close up.
Randy
jim simmons
Posts: 478 Joined: Sun Mar 09, 2003 10:37 pm
Location: Hillsboro Oregon
Contact:
Post
by jim simmons » Thu Aug 28, 2003 8:36 pm
Thank you so much, Randy. You did me a great favor, and probably several other people also.
Jim