Post by Stuart Clayman »

I went to a demo last week for the Kaiser-Lee board and Petra mentioned Primo Primer. The benefits are no sticking ..... =D> ... and after it is used you brush it off and recoat the shelf.. no scraping and no ugly buildups.

What is people's experience with it?

I assume it is a 5 to 1 ration with mixing..

Stuart
lissa
Posts: 84
Joined: Tue Jun 03, 2003 8:29 pm
Location: North Carolina
Contact:

Post by lissa »

Bert posted this not long ago