Post by daffodildeb »

I've seen some pendants with designs in black on dichro, and I'm wondering how it was done. I'm not referring to the decal type, or the pre-made dichro strips. The kind I'm asking about are individually done.

Somewhere I thought I saw a thread (probably another forum) about using black Sharpie pens to draw, and whatever was marked would fire in black. Was I dreaming? Or is there a way to do this?
Deb
Jack Bowman
Posts: 127
Joined: Mon Mar 17, 2003 10:52 pm
Location: Utah
Contact:

Post by Jack Bowman »

You were dreaming sort of. Another poster described a method of drawing a design in sharpie or whatever on the dichro, recoating the drawing and then puting the etching cream on. The dichro survives under the sharpie. I tried it and it works great.

To have a black design I use my dremel to grind away the design. Also works great. So does sandblasting.

One for a positive design and one for a negitive design.

Jack
Denise M.

Post by Denise M. »

Hi, Deb,

Black Sharpie burns off. However, someone did tell me that it's possible to have custom patterns printed on dichro. Maybe if you contacted Coatings By Sandburg someone there could be of help. Good luck.

Denise[/url]
Lisa Allen
Posts: 212
Joined: Sun Mar 09, 2003 3:23 pm
Location: Memphis, TN
Contact:

Post by Lisa Allen »

I don't know about the sharpie thing.......I can't imagine that working.

But, if you get a sheet of dichro on black glass, you can use resist to introduce a pattern then sandblast the dichro off, leaving you with the base black glass as the design surrounded by the dichro.

Lisa
Lisa Allen
http://www.lisa-allen.com
Today's mighty oak is just yesterday's nut that held its ground.
daffodildeb
Posts: 125
Joined: Mon Jul 28, 2003 3:48 am
Location: Hot Springs Village, AR

Post by daffodildeb »

Jack, by Jove--I think you've got it! :D

Thanks for clearing the mystery up!
Deb
Kitty
Posts: 444
Joined: Sun Mar 09, 2003 4:12 pm
Location: Gig Harbor, WA

Post by Kitty »

there used to be a jewelry maker in hawaii who put their designs on pendants and earrings. it was done with a computer program and an XY plotter which cut the stencils. the little stencils were adhesive-backed. she put them on her glass, sandblasted the dichro off, and fire polished. i know another jewelry maker who uses the same program and plotter to cut resist stencils for sandblasting images into stone he uses in his pieces.
Jack Bowman
Posts: 127
Joined: Mon Mar 17, 2003 10:52 pm
Location: Utah
Contact:

Post by Jack Bowman »

Kitty wrote:there used to be a jewelry maker in hawaii who put their designs on pendants and earrings. it was done with a computer program and an XY plotter which cut the stencils. the little stencils were adhesive-backed. she put them on her glass, sandblasted the dichro off, and fire polished. i know another jewelry maker who uses the same program and plotter to cut resist stencils for sandblasting images into stone he uses in his pieces.
I just spent a few weeks in Whistler BC with a couple who use a plotter to cut their sandblast resist. $10,000 for the plotter. It does extremely fine work.

Jack
Kitty
Posts: 444
Joined: Sun Mar 09, 2003 4:12 pm
Location: Gig Harbor, WA

Post by Kitty »

my friend's plotter wasn't anywhere near that much money. it does very precise work, too. i think he and the other person i referred to had the same equipment.
Paul Tarlow
Posts: 344
Joined: Sun Mar 09, 2003 4:06 pm
Location: Helios Kiln Glass Studio - Austin
Contact:

Post by Paul Tarlow »

Lisa Allen wrote:I don't know about the sharpie thing.......I can't imagine that working.

But, if you get a sheet of dichro on black glass, you can use resist to introduce a pattern then sandblast the dichro off, leaving you with the base black glass as the design surrounded by the dichro.

Lisa
Sharpie does work. The edges aren't as crisp as it is if you mask with masking tape or stickers.

Here's an example using a sticker (Michael's has a jillion tiny stickers to choose from for this kind of thing):

Image

Put the sticker on the dichro, brush on the etch, wait a couple minutes and rinse.

- Paul
daffodildeb
Posts: 125
Joined: Mon Jul 28, 2003 3:48 am
Location: Hot Springs Village, AR

Post by daffodildeb »

Oooh Paul. Now I know what all those sticker aisles at Michaels are for! And to think when my kids were growing up (a million years ago), all we had were stars! :cry:

THANKS--GREAT IDEA!! :D
Deb
Jim Wixon
Posts: 35
Joined: Sun Mar 09, 2003 3:50 pm
Location: Seal Beach

Post by Jim Wixon »

A black sharpie pen can be used as a resist. Draw a positive or negative design on the dichroic with a good black sharpie. apply the etch cream wash in water and it works! The catch is to experimennt with the amount of time that the etch cream is left on. Depending on the dichroic, the strength of the etch cream and the design, the time can be between 15 and 40seconds. Test strips should be done.
The results can be from a variation in the dichro hue to a clean image(not as sharp as a cut stencil) and the most useful a 'distressed' look.
jim
Peg
Posts: 74
Joined: Tue Apr 08, 2003 7:50 am
Location: Bristol, UK

Post by Peg »

OK, I gotta ask - what is a 'sharpie'?
No doubt it is called something else in the UK. Can we have a picture?
Paul Tarlow
Posts: 344
Joined: Sun Mar 09, 2003 4:06 pm
Location: Helios Kiln Glass Studio - Austin
Contact:

Post by Paul Tarlow »

Peg wrote:OK, I gotta ask - what is a 'sharpie'?
No doubt it is called something else in the UK. Can we have a picture?
Image

http://www.officedepot.com/ddSKU.do?level=SK&id=142364
J. Savina
Posts: 18
Joined: Thu Mar 27, 2003 2:28 pm
Location: DeMotte, Indiana
Contact:

Post by J. Savina »

Wow Jack, that must have been a really big plotter. My husbands plotter cost less than $2000.00 and he got the whole kit and cabootle, with patterns and vinyl and videos etc. He makes all my stencils for my etched dichroic designs, and he uses it for stencils for his sandblasted glass art.
The possibilities are endless
charlie
Posts: 961
Joined: Mon Mar 10, 2003 3:08 pm

Post by charlie »

there's lots of places that do custom etching patterns on dichro. there's a guy in glendale arizona that does the one's that sara uses. info in the old archives.
Jack Bowman
Posts: 127
Joined: Mon Mar 17, 2003 10:52 pm
Location: Utah
Contact:

Post by Jack Bowman »

The plotter

Not sure what it is and it's the only one I've seen while it is working. $10,000 CAN would be about $7200 US. He has another one that he paid a couple thousand for. I know it's about 40" wide and spits out stencil about as fast as you can see. Also scribes metal sheet though I'm not sure that's in the directions.

Also not sure he got a cabootle with it.
:roll:

I've seen water jet cut patterns in dichro. Anybody know any sources?

Jack
Dolores
Posts: 106
Joined: Mon Jul 14, 2003 9:21 pm
Location: Sunny Southern California
Contact:

Post by Dolores »

Pacific Art Glass in Gardena, California does water jet dichro patterns. Unfortunately, their website doesn't have any pics, but I've seen them at the shop and they are very interesting. They will also do custom work. They can be contacted at: 1-800-354-5277. :D
Kitty
Posts: 444
Joined: Sun Mar 09, 2003 4:12 pm
Location: Gig Harbor, WA

Post by Kitty »

plotter/stencil cutters start around $700 for desktop versions, and keep going up. if interested, see products made by STIKA ROLAND. Model SX-8 is the least expensive. i know somebody who's using this one, and it is pretty remarkable. it uses material about 12" wide, on a roll. Corel Draw works with it.
Dolores
Posts: 106
Joined: Mon Jul 14, 2003 9:21 pm
Location: Sunny Southern California
Contact:

Post by Dolores »

I just found a company through Google who are advertising a STIKA ROLAND SX-8 for only $429.00. http://specialdelivery.bizhosting.com/r ... tters.htmlDoes this machine really work well on all kinds of dichro (excluding textures, of course)? Is there any limit as to the amount or intricacy of the pattern that can be cut on any given page? My apologies to those of you who are experts at this technology, but this is the first time I've heard of this machine. I've been hand-etching designs with my dremel till my fingers have gone numb and this sounds like an investment worth making. Any experienced cutters out there who can offer some advise?

DOLORES
Dolores
Posts: 106
Joined: Mon Jul 14, 2003 9:21 pm
Location: Sunny Southern California
Contact:

Post by Dolores »

Opps! I did that URL wrong.
http://specialdelivery.bizhosting.com/r ... tters.html
If it didn't work this time, I give up!
:oops: