I just fused a piece of bullseye and I ended up with a small area of devit. I was wondering if any of  you have tried to use super spray on the devit and slump at the same time? 
Would I be better off coating with super spray and going back to full fuse then slumping in another firing? 
I did not put any spray on the first fuse. Thanks for your help.
			
			
									
						
										
						slumping and super spray
Moderators: Brad Walker, Tony Smith
- 
				Jerry Barnett
- Posts: 55
- Joined: Wed Mar 12, 2003 11:40 am
- Location: Texas, USA
I have not tried doing both at the same time, but do not believe it would be successful.  Even though the maturation range of Super Spray is stated as being 1300 to 1700, I have never heard a report of Super Spray maturing at a temperature in the lower part of the range.  I take the glass back to fusing temperatures when I use Super Spray.  Jerry
			
			
									
						
										
						slumping and super spray
I agree with Jerry. We have tried using super spray while slumping Spectrum, and it does not get hot enough at slumping temperatures. You will have to fire to fusing temp.