Super Spray
Moderators: Brad Walker, Tony Smith
-
- Posts: 9
- Joined: Thu Jul 10, 2003 10:12 am
- Location: Grand Rapids, Michigan
Super Spray
I purchased a bottle of "Super Spray" by FuseMaster. I also purchased a small spray bottle. The Super Spray is so thick it wrecked the spray bottle and froze it up the works before anything came out. What did I do wrong? What do the rest of you use to "Spray" "Super Spray"? I stopped before I wrecked another spray bottle with 975 Back Magic. It apears to be at least as thick as SS.
Paul F. Jackson
Looking Glass Studio
"What are you looking at?"
Looking Glass Studio
"What are you looking at?"
-
- Posts: 212
- Joined: Sun Mar 09, 2003 3:23 pm
- Location: Memphis, TN
- Contact:
I use a little Badger from Michael's that uses canned air as a propellant. I find it odd that your SS is thick though. I have a few bottles and all of them are pretty liquidy..... ![Think :-k](./images/smilies/eusa_think.gif)
![Think :-k](./images/smilies/eusa_think.gif)
Lisa Allen
http://www.lisa-allen.com
Today's mighty oak is just yesterday's nut that held its ground.
http://www.lisa-allen.com
Today's mighty oak is just yesterday's nut that held its ground.
-
- Posts: 340
- Joined: Mon Mar 10, 2003 4:16 pm
- Location: Northern CA
- Contact:
-
- Posts: 9
- Joined: Thu Jul 10, 2003 10:12 am
- Location: Grand Rapids, Michigan
The place I bought SuperSpray and 975 Back Magic from sent me an email. These products are not intended to be "sprayed" with a "spray" bottle. I'm supposed to use an airbrush which uses a compressor or canned air. They suggested using a brush. Seems like they should say that on the bottle or something. Perhaps they could re name the product "Super Brush On" ![Rolling Eyes :roll:](./images/smilies/icon_rolleyes.gif)
![Rolling Eyes :roll:](./images/smilies/icon_rolleyes.gif)
Paul F. Jackson
Looking Glass Studio
"What are you looking at?"
Looking Glass Studio
"What are you looking at?"
-
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
-
- Posts: 340
- Joined: Mon Mar 10, 2003 4:16 pm
- Location: Northern CA
- Contact: