Looks like someone figured it out!
http://seattletimes.nwsource.com/html/a ... st160.html
Photosensitive Glass
Moderators: Brad Walker, Tony Smith
-
Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
-
PDXBarbara
- Posts: 292
- Joined: Sun Mar 09, 2003 4:09 pm
- Location: Portland, OR
Went to the demo put on by Olympic Color Rods during GAS....John Leggot (Gaffer Glass) led the demo at Chihuly's boathouse studio. The photosensitive currently only comes in rods. but there was talk of sheet too, down the road. Rod (Gaffer Ruby) is $70/kg. (2.2lb/kg). They also have Reichenbach photosensitive glass....rods only...
yellow is $46/kg; gold ruby $43 ; copper ruby (not priced).
Yo Els! How was Boise?
Barbara
yellow is $46/kg; gold ruby $43 ; copper ruby (not priced).
Yo Els! How was Boise?
Barbara