After watching Avery's demo at WGW I'm convinced I need a muller. All the ones that I'm finding online seem outragously expensive.
Other than making one myself, any ideas where to get one cheap?
Thanks,
Paul
Other than making one myself, any ideas where to get one cheap?
Thanks,
Paul
-
Avery Anderson
- Posts: 86
- Joined: Sun Mar 09, 2003 6:21 pm
- Location: Cheshire. Oregon
- Contact:
Paul:
There was a glass blower at my presentation who said he was going to produce some mullers...he thought they would be fairly simply to make. I'm sorry...I forgot his name, but perhaps he will chime in.
Also, some people suggested getting a rod and just grinding the end. Probably would work.
Avery
There was a glass blower at my presentation who said he was going to produce some mullers...he thought they would be fairly simply to make. I'm sorry...I forgot his name, but perhaps he will chime in.
Also, some people suggested getting a rod and just grinding the end. Probably would work.
Avery
-
Alecia Helton
- Posts: 108
- Joined: Mon Aug 25, 2003 12:35 am
- Location: outside of Dallas TX
muller
For those of us who didn't make it to WGW, what is a muller?
Thanks,
Alecia
Thanks,
Alecia
Alecia Helton
Wear Original Wonders!
Carrollton TX
Wear Original Wonders!
Carrollton TX
-
Ron Coleman
- Posts: 468
- Joined: Sun Mar 09, 2003 3:20 pm
- Location: Columbus, Ohio USA
Re: muller
Used for mixing glass paints with a mediumAlecia Helton wrote:For those of us who didn't make it to WGW, what is a muller?
Thanks,
Alecia
http://www.art-boards.com/Muller's.htm
Ron
-
Paul Tarlow
- Posts: 344
- Joined: Sun Mar 09, 2003 4:06 pm
- Location: Helios Kiln Glass Studio - Austin
- Contact:
Re: muller
yup - those are the ones I found -- maybe its me but they seem outragously expensive for what they areRon Coleman wrote:Used for mixing glass paints with a mediumAlecia Helton wrote:For those of us who didn't make it to WGW, what is a muller?
Thanks,
Alecia
http://www.art-boards.com/Muller's.htm
Ron
btw Ron, it was good to see you this past weekend
-
Ron Coleman
- Posts: 468
- Joined: Sun Mar 09, 2003 3:20 pm
- Location: Columbus, Ohio USA
Re: muller
PaulPaul Tarlow wrote:After watching Avery's demo at WGW I'm convinced I need a muller. All the ones that I'm finding online seem outragously expensive.
Other than making one myself, any ideas where to get one cheap?
Thanks,
Paul
Look for a beer glass with a heavy bottom and grind it flat or look for a glass spice jar with a ground glass lid. Pitch out the jar and use the lid upsidedown.
http://fantes.com/images/98334spice.jpg
Ron
Ron
-
Ron Coleman
- Posts: 468
- Joined: Sun Mar 09, 2003 3:20 pm
- Location: Columbus, Ohio USA
-
Paul Tarlow
- Posts: 344
- Joined: Sun Mar 09, 2003 4:06 pm
- Location: Helios Kiln Glass Studio - Austin
- Contact:
-
Ron Coleman
- Posts: 468
- Joined: Sun Mar 09, 2003 3:20 pm
- Location: Columbus, Ohio USA
SHoot guys, How's $15 plus shipping sound. Soda Lime (actually Spectrum 96, so in a pinch you can melt it down) Ground to 80 grit. Can do 220 easy as well. Of course Latticino handles, and imitation marital aids would cost extra. Can probably crank about 4 an hour.
Since I've never used one, there might be tech specs that I can't imagine. Enlighten me...
Greg
Since I've never used one, there might be tech specs that I can't imagine. Enlighten me...
Greg
-
Brian and Jenny Blanthorn
- Posts: 353
- Joined: Mon Mar 10, 2003 5:25 pm
- Location: UK
- Contact:
The pics are a nice designwatershed wrote:SHoot guys, How's $15 plus shipping sound. Soda Lime (actually Spectrum 96, so in a pinch you can melt it down) Ground to 80 grit. Can do 220 easy as well. Of course Latticino handles, and imitation marital aids would cost extra. Can probably crank about 4 an hour.
Since I've never used one, there might be tech specs that I can't imagine. Enlighten me...
Greg
U do need 2 keep a heavy bace
With a slight round on the edge
No bubbles in the bace grind area
Soda lime is Ok
Clear best
U could cast one urself from scrap with a clear bace
Just a round thick pebble form is OK
If they get big they R hard 2 move

-
Elizabeth in UK
- Posts: 14
- Joined: Sat May 03, 2003 9:10 am
- Location: Bournemouth - England
- Contact:
I just did a search for "glass muller" in UK and got several hits.
Looking at
http://www.lawrence.co.uk/shop/index.ht ... g43_0.html
It seems to be a tool also used in printing so a printmakers supplier may be less expensive a supplier and easier to find than a specific glass supplier.
Looking at
http://www.lawrence.co.uk/shop/index.ht ... g43_0.html
It seems to be a tool also used in printing so a printmakers supplier may be less expensive a supplier and easier to find than a specific glass supplier.
Re: muller
You can find them at the flea markets pretty easily here in Ohio. The guys who wear them usually have sleeveless T-shirts and a big belt buckle. Wait, maybe I'm confusing the word with something else. Never mind.Alecia Helton wrote:For those of us who didn't make it to WGW, what is a muller?
Thanks,
Alecia
-
scooter riegelsperger
- Posts: 26
- Joined: Fri Mar 14, 2003 9:23 am
- Location: Houston,TX
- Contact:
muller makin
Paul,
I'll make you one for a discount on your next adv. powders class in Austin. Just give me a sketch of what you want & I will make it and lap it flat in whatever grit you want.
Robert
I'll make you one for a discount on your next adv. powders class in Austin. Just give me a sketch of what you want & I will make it and lap it flat in whatever grit you want.
Robert
Do illiterate people get the full effect of alphabet soup?
-
Barbara Muth
- Posts: 382
- Joined: Sun Mar 09, 2003 8:10 pm
- Location: Washington DC Metropolitan Area
- Contact:
from my notes it appears that another source for mullers are the folks who are reproducing older arts, like the folks at iconofile who have the least expensive muller I was able to find online... Here is an excerpt from my notes:
.........................................................
Least expensive glass muller found online:
http://iconofile.com/search_results.asp ... fromSearch
other glass mullers:
http://www.dickblick.com/zz049/73/produ ... ig_id=6184
http://www.danielsmith.net/cgi-bin/sgin ... 85=Y&GENP=
http://www.stainedglassstylists.com/cat ... 862964.htm
http://www.stainedglassstylists.com/cat ... oducts.htm
These folks sell a granite muller (wonder what that would be like?):
http://www.manuscriptarts.net/art_supplies.htm
..................................
Hey Ron, did it cost you as much to cast (when you figure in time and energy costs) as it would have to buy it?
still planning to get one....
Barbara
.........................................................
Least expensive glass muller found online:
http://iconofile.com/search_results.asp ... fromSearch
other glass mullers:
http://www.dickblick.com/zz049/73/produ ... ig_id=6184
http://www.danielsmith.net/cgi-bin/sgin ... 85=Y&GENP=
http://www.stainedglassstylists.com/cat ... 862964.htm
http://www.stainedglassstylists.com/cat ... oducts.htm
These folks sell a granite muller (wonder what that would be like?):
http://www.manuscriptarts.net/art_supplies.htm
..................................
Hey Ron, did it cost you as much to cast (when you figure in time and energy costs) as it would have to buy it?
still planning to get one....
Barbara
-
Rebecca M.
- Posts: 126
- Joined: Fri Sep 12, 2003 12:15 pm
- Location: Myrtle Beach
- Contact:
muller
I thought the granite muller would be like a mortar and pestle type thing.
I was going to try this out, but haven't gotten around to finding the one I
know is around here somewhere.....
I bought a small one from Sunshine. Looking in the price list from their catalog,
Glass Mullers
2" - 26.99
3" - 37.39
4" - 47.59
Not too bad considering some other prices out there.
http://www.sunshineglass.com
I was going to try this out, but haven't gotten around to finding the one I
know is around here somewhere.....
I bought a small one from Sunshine. Looking in the price list from their catalog,
Glass Mullers
2" - 26.99
3" - 37.39
4" - 47.59
Not too bad considering some other prices out there.
http://www.sunshineglass.com
-
Cynthia
Ed Hoy sells a 2" and a 4" glass muller. < $17.00 and < $30.00 respectively. Item numbers 7404 and 74041. If they carry them at these prices wholesale, then there are others out there, scads I would expect, for about that same price. Many painters grind their own pigments, so there are mullers out ther at the art supply houses. Look there as well.
http://www.edhoy.com
http://www.edhoy.com
When I saw mention of glass mullers, I thought it meant "mullers for glass", but now I see they are mullers MADE of glass. The ones on the link I followed said they were made for grinding pigments. Do these really hold up grinding glass, which I would presume is harder than most pigments? I would think that would depend on whether the muller glass or the enamel glass were harder. If the glass wears off, is contamination from the glass in the muller cause any problems in the enamel?
-
Barbara Muth
- Posts: 382
- Joined: Sun Mar 09, 2003 8:10 pm
- Location: Washington DC Metropolitan Area
- Contact:
Apparently not enough glass comes-off the muller to make a difference in your pigment. I'll bet I get more steel from my palette knife in the pigment than glass from the muller. One palette knife that I prepare enamel with (when not mulling) is old, its paper thin at the blade and has a weird shape from being ground away on the glass palette.Mark Kemp wrote:When I saw mention of glass mullers, I thought it meant "mullers for glass", but now I see they are mullers MADE of glass. The ones on the link I followed said they were made for grinding pigments. Do these really hold up grinding glass, which I would presume is harder than most pigments? I would think that would depend on whether the muller glass or the enamel glass were harder. If the glass wears off, is contamination from the glass in the muller cause any problems in the enamel?