Its been a very long time since I used an irid glass in any of my work. I'm getting ready to do a piece with it and although I do remember how easily the irid chips along the edge when cutting, I do not remember if I had more success with preventing the chipping by scoring the glass on the irid side or on the back. Anyone who cuts a lot of it please tell me which side you score on.
Thanks!
Amy
Cutting irid
Moderators: Brad Walker, Tony Smith
-
Amy on Salt Spring
- Posts: 270
- Joined: Sun Mar 09, 2003 5:43 pm
- Location: British Columbia, Canada
- Contact:
I score on the irid surface, but chips are unimportant to me because I'm always blasting a border off anyway. Doug Randall just showed me a neat trick. The surface of BE sometimes has a hard "skin" and it can be easier to score on the back of the sheet.
Clear as mud?
Brock
Clear as mud?
Brock
My memory is so good, I can't remember the last time I forgot something . . .
-
Terry Ow-Wing
- Posts: 124
- Joined: Sun Mar 09, 2003 3:21 pm
- Location: San Francisco, Ca.
- Contact:
-
Amy on Salt Spring
- Posts: 270
- Joined: Sun Mar 09, 2003 5:43 pm
- Location: British Columbia, Canada
- Contact:
Well it is Bullseye and as of yet I do not have a sandblasting setup so I guess I will try scoring on the back and see how it goes. I can grind the edges if it doesn't go well but its a large piece and that will be a lot of grinding so I want to minimize it if I can. Thanks,Brock wrote:I score on the irid surface, but chips are unimportant to me because I'm always blasting a border off anyway. Doug Randall just showed me a neat trick. The surface of BE sometimes has a hard "skin" and it can be easier to score on the back of the sheet.
Clear as mud?
Brock
-A
-
Amy on Salt Spring
- Posts: 270
- Joined: Sun Mar 09, 2003 5:43 pm
- Location: British Columbia, Canada
- Contact:
I just wanted to say that I have been scoring my Bullseye blue irid on the backside as Brock said Doug Randall recommended and its been breaking perfectly with no chipping. The little bit of grinding I've had to do has actually caused chipping whereas the cutting hasn't, go figure. Maybe I need a new head...and one for my grinder too.
Amy
Amy