OK this will involve your imagination.  Imagine a series of cast rings.  I want to pre cast the rings, polish etc.  Then put these rings inside a vessel form.  So you have a solid cast vase with rings inside.  
The trick is that I want the rings to be a different color from the vase.  They don't actually have to fuse to the vase, but I can imagine the machining to get the rings in IF I just cast them seperately.  
My idea is to cast the rings, then make the wax vase, fit the rings with frax paper  between the rings and the wax.  Then after it's in the plaster, the wax would go, the frax would be bonded to the plaster.  
Then when I fire it up, the frax paper would contain the rings while the mold fills with glass.  
I would love to have the rings contained and fill the mold hot, but I'm willing to settle for filling the mold with frit, to avoid the Void , reduce the stress on the frax from molten glass (the rings) on one side and a void on the other.  
Do I just have to submit to hours of dremel work, or is this possible?
Maybe I could use copper plates, but I still worry about leakage (and scale).  And the copper plates would be another design element.  
There are more ideas than time, but I'm focused on this one currently. 
Thank for your help
Greg
			
			
									
						
										
						Frax paper/ dams
Moderator: Brad Walker
- 
				rskrishnan
 - Posts: 14
 - Joined: Mon Aug 18, 2003 6:59 pm
 
Re: Frax paper/ dams
I think a rough sketch would do wonders - I'm all out of imagination and need a re-fill !!watershed wrote:OK this will involve your imagination. Imagine a series of cast rings. I want to pre cast the rings, polish etc. Then put these rings inside a vessel form. So you have a solid cast vase with rings inside.
The trick is that I want the rings to be a different color from the vase. They don't actually have to fuse to the vase, but I can imagine the machining to get the rings in IF I just cast them seperately.
My idea is to cast the rings, then make the wax vase, fit the rings with frax paper between the rings and the wax. Then after it's in the plaster, the wax would go, the frax would be bonded to the plaster.
Then when I fire it up, the frax paper would contain the rings while the mold fills with glass.
I would love to have the rings contained and fill the mold hot, but I'm willing to settle for filling the mold with frit, to avoid the Void , reduce the stress on the frax from molten glass (the rings) on one side and a void on the other.
Do I just have to submit to hours of dremel work, or is this possible?
Maybe I could use copper plates, but I still worry about leakage (and scale). And the copper plates would be another design element.
There are more ideas than time, but I'm focused on this one currently.
Thank for your help
Greg
1. So is the vase a "solid vase" i.e. one big hunk of conical glass with the rings embedded within ??
2. Or are the rings on the outside of the vase and the vase itself is hollow ??
Option #1 is a LOT of work/trouble chances of crakcs appearing are HIGH to say the least - but it would be COOL !!!
Option #2 is decidely easier but a whole order of magnitude less cooler!
And then there's probably option #3 ==> what you originally had envisions which simply did not make it's way to my grey matter.
Krishnan
--
If I could I would, but I can't so I won't.
Still I love to cast glass ....
			
						If I could I would, but I can't so I won't.
Still I love to cast glass ....
Kind of a cross between 2-3.  A cast vase, with rings inside Hoizantally, kind of like clunky RISD rings.  The more I think about it I may have to do it hot.  Hey, there's an analogy.  There's a child's toy that has various colored plastic rings, that you put on a post in size order.  If I wanted to put those in a vase form, but keep their colors from mixing with the vase color.  
Greg
			
			
									
						
										
						Greg
- 
				charlie holden
 - Posts: 260
 - Joined: Thu Mar 13, 2003 8:26 pm
 - Location: Atlanta
 
- 
				jerry flanary
 - Posts: 158
 - Joined: Tue Sep 09, 2003 11:11 pm
 - Location: norfolk, va