Here are two niew pieces just finished for your perusal....
http://aryana2.com/images/cinnamon.jpg
http://aryana2.com/images/flattery_web.jpg
Thanks for looking,
Aryana
New Pieces
Moderator: Brad Walker
-
Aryana B. Londir
- Posts: 8
- Joined: Sun Mar 09, 2003 11:22 pm
- Location: Cave Creek, AZ
- Contact:
-
Aryana B. Londir
- Posts: 8
- Joined: Sun Mar 09, 2003 11:22 pm
- Location: Cave Creek, AZ
- Contact:
Thank you very much for your compliments. "Flattery" is an 11" triangle slumped in a shallow mold. It is comprised of three pieces joined together on a clear base with pattern bars, full fused, then tack fused with stringers and gold dots. "Cinnamon" is 16" high x 6" wide, made with frit wafers which were full fused onto the top and bottom pieces. Addiional frit applied and tack fused. The center portion was a lot of frit tack fused onto two layers. The stand was made by Dick Kolpak, and has iron spacers to divide the sections.